90 and 96 coe Q

Use this forum for discussion on kiln casting, pate de verre, and related topics.

Moderator: Brad Walker

Post Reply
rodney
Posts: 167
Joined: Mon Mar 10, 2003 12:05 pm
Location: new mexico
Contact:

90 and 96 coe Q

Post by rodney »

is there a difference in the way 90 and 96 coe frit fires,,,,what are the difference,,,thanks,,rodney
Tim Lewis
Posts: 35
Joined: Sun Mar 09, 2003 10:56 pm
Location: Western NC
Contact:

Post by Tim Lewis »

Each glass has it own formula so even different glasses with the same COE can melt differently, especially different viscoity.