Fusing schedules- ASAP

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Chris - L.I.
Posts: 3
Joined: Tue May 13, 2003 11:18 pm

Fusing schedules- ASAP

Post by Chris - L.I. »

Where should I be finding these? I want to contour fuse 2 inch squares of 96. It is 2 layers of glass, white on the bottom and clear irridized on top with a samll black graduation cap on top. Please help me so I can start on these as I have to make about 100 before AUg. 2nd. Thank you so much.

Chris - L.I.
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Post by Brad Walker »

For System 96 schedules, click on the link to the System 96 website at the top of this page.

For Bullseye, Uroboros, or Wasser schedules, click on the respective links, also at the top of the page.

Once you get the the website, just look for the section of their sites with the firing schedules. All of the major manufacturers have that information online.