big kiln -vs- little kiln
Moderators: Brad Walker, Tony Smith
big kiln -vs- little kiln
I have been quite succesfully using my paragon PMC kiln (about 8X8X8) with fiberboard shelves for small fusing for a year or so. NO failures. So I get a larger glass paragon glass kiln (13X9) with ceramic shelves. it's the same controller. using the same program or going up even slower, my glass is breaking into numerous pieces. for instance a 1X2" piece might be in 6-8 pieces. Anyone have any suggestions?
-
- Posts: 148
- Joined: Tue Mar 11, 2003 12:04 pm
- Location: Houston Tx
- Contact:
-
- Site Admin
- Posts: 1528
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact: