If I fire the paints at 1480, how long max can I hold there and not lose the color. I would like to paint and then full fuse, three layers of glass with the paints on the top layer only.
Susan W
Paradise paints temp
Moderators: Brad Walker, Tony Smith
-
Susan Wright
- Posts: 38
- Joined: Tue Mar 11, 2003 11:56 am
- Location: Corpus Christi, TX,KCMO, Great Lakes
- Contact:
-
Amy Schleif-Mohr
- Posts: 280
- Joined: Sun Mar 09, 2003 5:18 pm
- Location: Milwaukee
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Paradise paints temp
SusanSusan Wright wrote:If I fire the paints at 1480, how long max can I hold there and not lose the color. I would like to paint and then full fuse, three layers of glass with the paints on the top layer only.
Susan W
I never used Paradise paints, but I would suggest that you just go for it. Fire until you see that you have the fuse that you want and hope that the enamels follow along. I think that they should.
Bert
Re: Paradise paints temp
i don't know, but it will depend upon the color(s) you're using. the red, yellow, and orange (ROY) will burn out faster than the others. you might pm avery, who uses these a lot.Susan Wright wrote:If I fire the paints at 1480, how long max can I hold there and not lose the color. I would like to paint and then full fuse, three layers of glass with the paints on the top layer only.
Susan W
-
Susan Wright
- Posts: 38
- Joined: Tue Mar 11, 2003 11:56 am
- Location: Corpus Christi, TX,KCMO, Great Lakes
- Contact:
I just did one test fire. I am using a water medium 1544 at this time. I am trying to cut out multible firings if I can but so far I'm not getting the look I'm after mainly because of some problems not having to do with the paints.
I am fusing the base layers first and then cutting with the Taurus into the shape. sandblasting some details, painting some and then taking to a full fuse. The test showed that I wasn't getting the depth of color I want, splotchy somewhat which I'm sure is a technique problem but to resolve, I'm going to try another quick fire to 1480 and an immediate cut off.
I am fusing the base layers first and then cutting with the Taurus into the shape. sandblasting some details, painting some and then taking to a full fuse. The test showed that I wasn't getting the depth of color I want, splotchy somewhat which I'm sure is a technique problem but to resolve, I'm going to try another quick fire to 1480 and an immediate cut off.