My name is Jianu Vladimir and I am a Romanian artist working in pâte de verre. I face some problems that I have been trying to solve on my own for about one year now but with no significant progress and I hope that someone more experienced than me might help me.
My most important problem is that the heat resistant plaster that I use for the molds cracks and thus leads to the appearance of lines on the models. I use a mix of gypsum and very finely grinded heat resistant bricks and I would like to find another solution for the heat resistant plaster (another recipe). In exchange for a useful recipe I can make (and send to you) an artistic model of your choice style “Art Nouveau”.
Thank you very much for your time, I remain at your disposition for any additional information.
Pâte de verre
Moderators: Brad Walker, Tony Smith
-
Glenda Kronke
- Posts: 64
- Joined: Tue Mar 11, 2003 11:44 am
- Location: Austin, TX
- Contact:
Mold recipe
Jianu,
I don't think you need to bribe anyone for their mold recipes (although, I am sure many would love to recieve one of your pieces!!) .
Look in the Kiln Casting forum for lots of discussion on recipes for molds. I am sure one of the casters will be more than helpful. I don't cast glass myself, but I am interested in this process and am trying to talk myself into taking a mold making class. From everything I have read, there seems to be so much to learn just about mold making that I am thinking it is as much of an art as casting the glass!
Give these guys a day or two and you will probably have more recipes than you can handle.
Good luck!
glenda
I don't think you need to bribe anyone for their mold recipes (although, I am sure many would love to recieve one of your pieces!!) .
Look in the Kiln Casting forum for lots of discussion on recipes for molds. I am sure one of the casters will be more than helpful. I don't cast glass myself, but I am interested in this process and am trying to talk myself into taking a mold making class. From everything I have read, there seems to be so much to learn just about mold making that I am thinking it is as much of an art as casting the glass!
Give these guys a day or two and you will probably have more recipes than you can handle.
Good luck!
glenda
An often used formula is 1 part pottery plaster to 1 part silica, mixed with water as usual. Here is an excellent web site for additional info:
http://www.glassaustralia.anu.edu.au/da ... .data.html
Select the "Pate de Verre" link.
Cheers,
Suzan
http://www.glassaustralia.anu.edu.au/da ... .data.html
Select the "Pate de Verre" link.