Yes I have been cleaning them. I have one of those old concrete wash tubs , I fill it with about a half inch of water and a couple of drops of Dawn dish soap. Then I give the earring a quick rub on the concrete to get the kiln wash off then rub the earring between my fingers to clean it. Then a quick rinse and it's done.
Randy
How Do YOU apply E 6000
Moderators: Brad Walker, Tony Smith
-
K Okahashi
- Posts: 49
- Joined: Mon Mar 10, 2003 7:29 pm
- Location: Washington
One good source of jewelry cards, etc I have found is: http://www.fetpak.com/
For a fraction of the cost you'll get some really nice looking hang tags.
Good luck!
For a fraction of the cost you'll get some really nice looking hang tags.
Good luck!
randy -- you might like to add some alumina hydrate to your kilnwash. my earrings only stick to my kaolin/alumina hydrate kilnwash if they get too hot, like 1600. my small kiln doesn't have a controller, only pyrometer, so sometimes if i get distracted or dont hear timer, it sails over 1490, which i find is the primo temp for dangle earrings. a little cooler for ones with surface texture (1450-1460), and about 1550 or so for dots.
if i need to clean up the backs of earrings for some reason, i like to use black waterproof sandpaper, 220 grit. a fourth of a sheet on the kitchen counter, wet, and the kilnwash comes off instantly, same as your rubbing it on concrete.
i have found that most colors don't need sanding before epoxy, but a couple of them seem to require it: they are the transparent oranges and yellows.
if i need to clean up the backs of earrings for some reason, i like to use black waterproof sandpaper, 220 grit. a fourth of a sheet on the kitchen counter, wet, and the kilnwash comes off instantly, same as your rubbing it on concrete.
i have found that most colors don't need sanding before epoxy, but a couple of them seem to require it: they are the transparent oranges and yellows.