[quote="Hugo Gavarini"]Hello;
But what effect did you get when blasting with SiC a colored glass surface, then firing. I believe I have read Steve got a microscopic pitting effect under a magnifier and a slight haze when seeing with the eye. Am I right?. BTW, pictures by Steve are good ones, I misread them.
On the subject of “pittingâ€
Eureka
Moderators: Brad Walker, Tony Smith
-
Steve Immerman
- Posts: 208
- Joined: Sun Mar 09, 2003 4:55 pm
- Location: Eau Claire, Wisconsin
- Contact:
-
Hugo Gavarini
- Posts: 49
- Joined: Mon Mar 10, 2003 12:03 pm
- Location: Patagonia Argentina
Re: Trying to isolate the culprit
"...As for color change, I'm not sure what you mean."
Steve,
I mean local decolorizing (Sp.?), a lack of color in the pit surrounding. I wonder if somehow the pit content have eaten the near matrix color.

Steve,
I mean local decolorizing (Sp.?), a lack of color in the pit surrounding. I wonder if somehow the pit content have eaten the near matrix color.
Hugo