release agent for between plaster

Use this forum for discussion on kiln casting, pate de verre, and related topics.

Moderator: Brad Walker

Post Reply
Leslie Ihde
Posts: 45
Joined: Wed Jun 04, 2003 9:02 pm
Location: Vestal, New York

release agent for between plaster

Post by Leslie Ihde »

I have a heavily carved plaster mold made from hydrocal. I want to made a reverse mold from it in a plaster /silica mix which can be fired under glass. I am thinking of using mold soap as a release agent. Has anyone done this with sucess? Any one have a better thought? I don't dare damage the original mold in order to produce it's reverse.

Thanks in advance
Leslie Ihde
Turning Point Studio
Vestal, New York
charlie holden
Posts: 260
Joined: Thu Mar 13, 2003 8:26 pm
Location: Atlanta

Post by charlie holden »

Thin clay slip will definitely work but you may lose too much detail. It seems to me that I've used Murphy's Oil Soap for this. That's what I usually use on my molds but I'm not generally pouring plaster against plaster. I'll have to check my slipcasting book back at my studio.
rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Post by rosanna gusler »

murphys oil soap works for me. maybe you will want to pull a latex type mold off your origonal so you can duplicate it if it gets damaged. rosanna
GlassOrchid
Posts: 57
Joined: Wed Apr 16, 2003 9:35 pm
Location: Maine
Contact:

Pourable latex?

Post by GlassOrchid »

I took a pate de verre class a year or so ago and the instructor mentioned using some pourable latex to make copies of the positive so one can make duplicates later... does anyone know what this stuff is actually called and where to get it?

Thanks,
Nancy
Sharon Lee
Posts: 13
Joined: Thu May 08, 2003 11:05 am
Location: Roseville, CA

Post by Sharon Lee »

Nancy, try this link http://www.clayartcenter.com/synairproducts_1.htm . I bought some mold making stuff from them but haven't tried it yet.
Sharon
Brad Walker
Site Admin
Posts: 1539
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Post by Brad Walker »

You can also use one of the liquid rubbers from a company like Smooth-On. Most are two parts, which are mixed together. They become rubber-like once they cure and can be used to make multiple wax duplicates of the original.

http://www.smooth-on.com
GlassOrchid
Posts: 57
Joined: Wed Apr 16, 2003 9:35 pm
Location: Maine
Contact:

Post by GlassOrchid »

Thanks both! How exciting...... That's exactly what I was looking for. This is the thing that makes me love working with glass.... there is always more to explore and learn... now the downside is that there are always more toys to buy.......

~Nan
Nikki ONeill
Posts: 169
Joined: Mon Mar 10, 2003 11:55 am
Location: Silver Spring, MD
Contact:

Post by Nikki ONeill »

Nan:
Alse try Polytek. They have a great, instructive catalog and make several kinds of rubber molds. They'll also send you smaller size containers at a discount, on a one-time per product basis so you can try them out. Have fun!
Nikki
Post Reply