Source for thin float glass
Moderators: Brad Walker, Tony Smith
-
Kopperwood
- Posts: 14
- Joined: Sat Mar 15, 2003 10:07 am
- Location: Asheville, NC
- Contact:
Source for thin float glass
Can anyone give me a source for thin float glass? I'm looking for something about half the thickness of regular 3/32 single strength. Just looking for a few sq ft for a prototype, then would need to buy 100 sq ft at a time.
-
Gale aka artistefem
- Posts: 184
- Joined: Sun Mar 09, 2003 8:14 pm
- Location: MO-on the banks of the Mississippi
- Contact:
I used to buy 1/16" from one of my Colorado wholesalers.
Sorry........ can't remember which one. It's been a very long time since I used it.
Check with:
D&L Stained Glass Supply, Inc.
4939 N. Broadway
Boulder, CO 80304
(800) 525-0940
(303) 449-8737
(303) 442-3429 (fax)
http://www.dlstainedglass.com
info@dlstainedglass.com
or
Artisans Wholesale Stained Glass, Inc.
666 Buchtel Boulevard
Denver, CO 80210-1547
(800) 525-9008
(303) 777-0161 (fax)
artisans@uswest.net
Sorry........ can't remember which one. It's been a very long time since I used it.
Check with:
D&L Stained Glass Supply, Inc.
4939 N. Broadway
Boulder, CO 80304
(800) 525-0940
(303) 449-8737
(303) 442-3429 (fax)
http://www.dlstainedglass.com
info@dlstainedglass.com
or
Artisans Wholesale Stained Glass, Inc.
666 Buchtel Boulevard
Denver, CO 80210-1547
(800) 525-9008
(303) 777-0161 (fax)
artisans@uswest.net
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Source for thin float glass
KopperwoodKopperwood wrote:Can anyone give me a source for thin float glass? I'm looking for something about half the thickness of regular 3/32 single strength. Just looking for a few sq ft for a prototype, then would need to buy 100 sq ft at a time.
Look for a picture frame supplier. They sell it in relatively small boxes at good prices.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Brian and Jenny Blanthorn
- Posts: 353
- Joined: Mon Mar 10, 2003 5:25 pm
- Location: UK
- Contact:
Re: Source for thin float glass
Also used 4 slide glass 35mmBert Weiss wrote:KopperwoodKopperwood wrote:Can anyone give me a source for thin float glass? I'm looking for something about half the thickness of regular 3/32 single strength. Just looking for a few sq ft for a prototype, then would need to buy 100 sq ft at a time.
Look for a picture frame supplier. They sell it in relatively small boxes at good prices.
Also microscope slides stuff