Cutting narrow strips
Can someone please tell me the best way to cut narrow strips of glass consistently? 1/8"-1/4" wide in both thin and standard thicknesses of glass.
Thanks
Thanks
1/4" strips in 3mm are easy enough, cut a series of 1/2" strips, score them, and split them with running pliers. 1/8" strips, in 3mm are much harder, as glass does not normally break at a width approaching it's thickness. You will be able to get 1/8" strips out of thin glass however.
My memory is so good, I can't remember the last time I forgot something . . .
-
judith
- Posts: 49
- Joined: Tue Mar 11, 2003 8:57 am
- Location: Vitrum Studio - Maryland - DC area
- Contact:
Brock is right (happens now and again) but I think one imortant fact should be added. When breaking glass, you'll have greater succes if you "divide and conquer" (I think Bob said that). By that I mean you should try to keep the width of the glass on either side of the score line the same.Brock wrote:1/4" strips in 3mm are easy enough, cut a series of 1/2" strips, score them, and split them with running pliers. 1/8" strips, in 3mm are much harder, as glass does not normally break at a width approaching it's thickness. You will be able to get 1/8" strips out of thin glass however.
For instance, if you want 1/4" strips, first cut your blank of glass roughly in half (the width of the piece you're cutting off sould be evenly divisible by 1/4" for minimum waste), then cut the half in half, then the resulting half in half, and so on, until you have a 1/2" strip. Then cut the 1/2" strip in half. Since there is an equal amount of glass on either side of the score, you'll have much greater success in having the break run down the score line. Works for me. I hope this makes sense.
judith
-
Stuart Clayman
- Posts: 224
- Joined: Mon Mar 31, 2003 12:35 pm
- Location: Virginia
- Contact:
Brock is right (happens now and again) . . .
Waah! Implcit criticism. Judy! Weren't you paying attention at BECon?
You can never, never, ever criticize someone. It's a rule. And, you didn't use the but/and convention. Brock
Waah! Implcit criticism. Judy! Weren't you paying attention at BECon?
You can never, never, ever criticize someone. It's a rule. And, you didn't use the but/and convention. Brock
My memory is so good, I can't remember the last time I forgot something . . .
Re a good strip cutter: Judith sells a great one. It may seem expensive but if you do a lot of strip cutting, you'll kick yourself for not having bought one before.
Re the comments on divide-n-conquer cheatin technology: I find it easier to make all the scores first and then break/run them. With 1/4" to 3/8" strips, break a group of 8, then run the middle one (2 groups of 4), etc.
Trying to get 1/8" wide strips out of 1/8" thick glass is an exercise in futility. Cut them out of the thin stuff and double them up.
Marty
Re the comments on divide-n-conquer cheatin technology: I find it easier to make all the scores first and then break/run them. With 1/4" to 3/8" strips, break a group of 8, then run the middle one (2 groups of 4), etc.
Trying to get 1/8" wide strips out of 1/8" thick glass is an exercise in futility. Cut them out of the thin stuff and double them up.
Marty
-
Bob
- Posts: 215
- Joined: Mon Mar 10, 2003 1:01 pm
- Location: Salt Spring Island, British Columbia
- Contact:
Hey Marty,
That's exactly the way that I do it... score first, break into groups of 8, then 4, then 2, and voila...finally nice even single strips. Perhaps at the upcoming WGW there could be a stripping contest. Brock starts off in one of his (dare I say) patented Hawaiian shirts and ....
Cheers,
Bob
That's exactly the way that I do it... score first, break into groups of 8, then 4, then 2, and voila...finally nice even single strips. Perhaps at the upcoming WGW there could be a stripping contest. Brock starts off in one of his (dare I say) patented Hawaiian shirts and ....
Cheers,
Bob
-
Jackie Beckman
- Posts: 475
- Joined: Sun Mar 09, 2003 5:01 pm
- Location: Arizona
- Contact:
Bob wrote:Hey Marty,
That's exactly the way that I do it... score first, break into groups of 8, then 4, then 2, and voila...finally nice even single strips. Perhaps at the upcoming WGW there could be a stripping contest. Brock starts off in one of his (dare I say) patented Hawaiian shirts and ....
Cheers,
Bob
Brock and Doug had a "strip-off" in Portland last year. If I remember correctly it was a tie. (sort of) One made longer strips from "evil white" while the other made thinner strips, but from a more "friendly" clear. No Hawaiian shirt that day, but it was fun to watch never the less.
Ok....I have to chime in here. I do have one of those big table model strip cutters, but for production cutting 1/4" to 3/8" theres nothing like the good old manual strip cutter, provided you do the right retooling with them.
And that damn dance keeps coming back to haunt me, but it is always fun at parties. But never as fun as the look on Brocks face at the transvestite show when the female impersonator came over to him and got him really nervous. What did she say to you...huh!. .....hahaha touche!
And that damn dance keeps coming back to haunt me, but it is always fun at parties. But never as fun as the look on Brocks face at the transvestite show when the female impersonator came over to him and got him really nervous. What did she say to you...huh!. .....hahaha touche!
. . . And that damn dance keeps coming back to haunt me, but it is always fun at parties. But never as fun as the look on Brocks face at the transvestite show when the female impersonator came over to him and got him really nervous. What did she say to you...huh!. .....hahaha touche!
I prefer to think that he/she just picked the hunka-hunka-burning-love looking guy out of the audience. Or maybe it was the shirt. And why do I seem to end up at those clubs in Portland? And who bought the picture, Doug?
I prefer to think that he/she just picked the hunka-hunka-burning-love looking guy out of the audience. Or maybe it was the shirt. And why do I seem to end up at those clubs in Portland? And who bought the picture, Doug?
My memory is so good, I can't remember the last time I forgot something . . .
Well, as you know Brock...Portland is a fun town, and we're fun people. So there you have it, that why you alway end up having fun when your here.... And yes, I bought four pictures Brock....Want one!Brock wrote:. . . And that damn dance keeps coming back to haunt me, but it is always fun at parties. But never as fun as the look on Brocks face at the transvestite show when the female impersonator came over to him and got him really nervous. What did she say to you...huh!. .....hahaha touche!
I prefer to think that he/she just picked the hunka-hunka-burning-love looking guy out of the audience. Or maybe it was the shirt. And why do I seem to end up at those clubs in Portland? And who bought the picture, Doug?
Well, as you know Brock...Portland is a fun town, and we're fun people. So there you have it, that why you alway end up having fun when your here.... And yes, I bought four pictures Brock....Want one!
Nah. I can remember it. Vividly. Brock
Nah. I can remember it. Vividly. Brock
My memory is so good, I can't remember the last time I forgot something . . .
Judith who? Details please!Marty wrote:Re a good strip cutter: Judith sells a great one. It may seem expensive but if you do a lot of strip cutting, you'll kick yourself for not having bought one before.
Re the comments on divide-n-conquer cheatin technology: I find it easier to make all the scores first and then break/run them. With 1/4" to 3/8" strips, break a group of 8, then run the middle one (2 groups of 4), etc.
Trying to get 1/8" wide strips out of 1/8" thick glass is an exercise in futility. Cut them out of the thin stuff and double them up.
Marty
Paul
Paul Bush
Flying Fish Studio
Portland, Oregon
Flying Fish Studio
Portland, Oregon
-
Barbara Muth
- Posts: 382
- Joined: Sun Mar 09, 2003 8:10 pm
- Location: Washington DC Metropolitan Area
- Contact:
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
I have a template technique where I cut a strip that is the width I want plus the distance from the wheel to the edge of the cutter. Seam the edges and then I place the strip to the right of my L square. I finger tip the alignment and then hand cut. This works for all size templates. For strip cutting I have one for the double size and half size.
Lo tech but accurate if you can make an accurate template.
Lo tech but accurate if you can make an accurate template.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
The Hobbyist
- Posts: 311
- Joined: Sun Mar 09, 2003 7:09 pm
- Location: Sun City West (NW Phoenix), AZ
- Contact:
Thanks Bert, I like lo-tech
Thanks Bert,
That's a great idea. Why didn't I think of that?
I like the lo tech, homemade methods. It leaves more money for glass.
Jim
That's a great idea. Why didn't I think of that?
I like the lo tech, homemade methods. It leaves more money for glass.