BORAX Qs,,,,,sprayer,,,recipe
Moderators: Brad Walker, Tony Smith
BORAX Qs,,,,,sprayer,,,recipe
does anyone have a suggestion for a spayer that wont get clogged with borax,,,,,,,,,also is there there a PERFECT mixture for the borax, is more better, is less better,,,,thanks,rodney
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
-
Paul Tarlow
- Posts: 344
- Joined: Sun Mar 09, 2003 4:06 pm
- Location: Helios Kiln Glass Studio - Austin
- Contact:
Re: BORAX Qs,,,,,sprayer,,,recipe
Here's the borax/klyr-fire/H20 recipe that I use:rodney wrote:does anyone have a suggestion for a spayer that wont get clogged with borax,,,,,,,,,also is there there a PERFECT mixture for the borax, is more better, is less better,,,,thanks,rodney
http://www.warmglass.com/basic/making_y ... htm#DEVIT2
Paul
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: BORAX Qs,,,,,sprayer,,,recipe
The sprayer I have used most is a mouth atomizer. Someimes described as a cheap thrill. Get it at the art supply store for a couple of bucks.rodney wrote:does anyone have a suggestion for a spayer that wont get clogged with borax,,,,,,,,,also is there there a PERFECT mixture for the borax, is more better, is less better,,,,thanks,rodney
I have a cheap badger sprayer that works for things like borax, kiln wash, and mica, assuming you have compressed air available.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions