How do I make a 1-piece shelf from a 3-pc. shelf?

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Pamela B.
Posts: 14
Joined: Tue Mar 11, 2003 11:05 am
Location: Tenmile OR

How do I make a 1-piece shelf from a 3-pc. shelf?

Post by Pamela B. »

I have a new Evenheat 2542 kiln with a three-piece shelf and would like to be able to make something larger than what each individual piece can accommodate. What is the best way to span the gap between pieces? A single sheet of fiberboard?

Pam
Lisa Allen
Posts: 212
Joined: Sun Mar 09, 2003 3:23 pm
Location: Memphis, TN
Contact:

Post by Lisa Allen »

I have a big Evenheat as well and cut those 3 shelves up for dams. I use a Unifrax HD 1 and 1/2" duraboard as a shelf instead, sitting right on the kiln floor......works just fine.

Lisa
Lisa Allen
http://www.lisa-allen.com
Today's mighty oak is just yesterday's nut that held its ground.
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Post by Marty »

ditto on kiln and solution.

Marty
Pamela B.
Posts: 14
Joined: Tue Mar 11, 2003 11:05 am
Location: Tenmile OR

Post by Pamela B. »

Thank you thank you thank for the suggestions. Now, why doesn't Evenheat suggest this solution? Or the distributor from whom I bought the kiln? What's the point to having a 3-piece shelf if one wants to make one big thing? Or, as was my intention, to make four 14" plates? Grrr.
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Post by Marty »

Don't forget to rigidize the board.