Does anybody know where I might begin to look for a larger draping mold than the 7" one that is available? I mean the one that is stainless steel and looks like a bar shaker or milksake machine cup.
Thanks,
Paulette
10" vase draping mold
Moderators: Brad Walker, Tony Smith
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: 10" vase draping mold
PaulettePaulette wrote:Does anybody know where I might begin to look for a larger draping mold than the 7" one that is available? I mean the one that is stainless steel and looks like a bar shaker or milksake machine cup.
Thanks,
Paulette
I made one with black iron pipe. I put a flange on the bottom for stability, and a cap on the top for shape and then covered it all with fiberfrax blanket, then tied it together with some nichrome wire.
The mold you were mentioning is a martini shaker. Much cheaoer at the restaurant supply than the glass mold store.
You could also come up with a way to raise the martini shaker up higher. Firebricks, plaster, castable,steel, whatever.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
I located a small ss ice bucket at a local dollar store and purchased it to use as a drape mold for glass. Fortunately my regular shaker mold fits over the base ot the ice bucket so I can telescope the two forms and get a taller drape mold. I never could find that ice bucket again. I'm still looking for another one.
Best wishes,
Tom in Texas
Best wishes,
Tom in Texas
-
Susan Slack
- Posts: 13
- Joined: Wed Apr 02, 2003 10:10 am
- Location: Green Oaks, Il.
Re: 10" vase draping mold
where did you get the flange? i can only find galvanized flanges at home depot.Bert Weiss wrote:
Paulette
I made one with black iron pipe. I put a flange on the bottom for stability, and a cap on the top for shape and then covered it all with fiberfrax blanket, then tied it together with some nichrome wire.
The mold you were mentioning is a martini shaker. Much cheaoer at the restaurant supply than the glass mold store.
You could also come up with a way to raise the martini shaker up higher. Firebricks, plaster, castable,steel, whatever.
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: 10" vase draping mold
Charliecharlie wrote:where did you get the flange? i can only find galvanized flanges at home depot.Bert Weiss wrote:
Paulette
I made one with black iron pipe. I put a flange on the bottom for stability, and a cap on the top for shape and then covered it all with fiberfrax blanket, then tied it together with some nichrome wire.
The mold you were mentioning is a martini shaker. Much cheaoer at the restaurant supply than the glass mold store.
You could also come up with a way to raise the martini shaker up higher. Firebricks, plaster, castable,steel, whatever.
Try a plumbing supply. I used black iron. Galvi is not good to heat up. The black iron protected by blanket fared well.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions