Depression Molds

Post by Paul Housberg »

Seeking any and all advice on making depression molds.

I need to make several one-shot molds varying in size, the largest roughly 10" x 20" by one to two inches deep. I'll be casting clear cullet or patties, probably Bullseye, but would welcome recommendations. (Have been perusing the archives, but specific tips for depression molds would be great.)

I've done this before but it's been many, many years. I believe I used 50/50 plaster/silica over a (wet) terra cotta form. I laid a piece of chicken wire in the wet plaster/silica for strength, though I wonder whether it made a difference. I got very little cracking, though for the work I'm doing, hairline cracking is not a problem. I don't recall my drying or firing schedule.

So, several questions:

I'd like to sculpt my positive in something firmer than terra cotta. I've used various grades of plastilene, but if I recall correctly, it didn't come out of the plaster as cleanly as the terra cotta. Thoughts?

What's the state of the art regarding plaster/silica mold recipes? I've read references to other materials such as Castalot which I'd be willing to try, but I haven't got the time for a lot of experimentation.

Any other advice, tips, cautions, etc. would be a big help: drying times, firing schedules, reinforcement, sources of info, etc.
Image
Paul Housberg
Glass Project, Inc.
Art Glass Feature Walls
http://www.glassproject.com
http://www.facebook.com/housberg
Don Burt
Posts: 580
Joined: Sun Mar 09, 2003 8:45 pm
Location: Bloomington, Indiana
Contact:

Re: Depression Molds

Post by Don Burt »

Paul Housberg wrote: clip
I've used various grades of plastilene, but if I recall correctly, it didn't come out of the plaster as cleanly as the terra cotta. Thoughts?
clip
I've sculpted relief stuff on glass sheet with plasticene. THen I smoothed it with a hair dryer to get it glossy. THen cast it on the glass plate using 50/50 mix Silica flour/plaster ( I forget the water %). The molds came off quite cleanly. Held up OK to 1385F firings.
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Post by Bert Weiss »

Paul

If you can get rubber positives they are the easiest way to make plaster negatives. Smooth-on makes dozens of rubber formulations. I like the one that has built in mold release. You could make a clay positive, a pure plaster negative and a rubber positive. Make it as thick as you want the mold to be. With no undercuts, you can simply pull up the rubber and the mold is ready to dry. Solid rubber is easier to work with than a thin coating of rubber with a plaster mother.

My take on plaster is to make a plaster/silica face coat, and back it up with a stiff mix including plaster , silica, grog, and chopped fibers. I use #2 casting plaster from the drywall supply place. I'm told that pottery plaster is not much different.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Nikki ONeill
Posts: 169
Joined: Mon Mar 10, 2003 11:55 am
Location: Silver Spring, MD
Contact:

Post by Nikki ONeill »

Paul:
Another technique you might want to consider is casting bllets in a box mold, creating a reverse felief. You would make a positive relief element in plaster and cast over it in a box. The method was taught and demonstratd by Ted Sawyer from Bullseye, and they now have a new TipSheet (#5) on the method. You can download the tipsheet from their site. The pieces done in our class using BE casting billets came out amazingly clear and needed little if any cold working. A key element is the use of a refractory wall mold made by screwing pieces of Skamol compressed vermiculite together. The mold is re-usable. A really interesting technique.
Nikki
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Post by Brad Walker »

Nikki O'Neill wrote:Paul:
Another technique you might want to consider is casting bllets in a box mold, creating a reverse felief. You would make a positive relief element in plaster and cast over it in a box. The method was taught and demonstratd by Ted Sawyer from Bullseye, and they now have a new TipSheet (#5) on the method. You can download the tipsheet from their site. The pieces done in our class using BE casting billets came out amazingly clear and needed little if any cold working. A key element is the use of a refractory wall mold made by screwing pieces of Skamol compressed vermiculite together. The mold is re-usable. A really interesting technique.
Bullseye is doing a demo on this at the upcoming Warm Glass Weekend conference.
jim simmons
Posts: 478
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Post by jim simmons »

Brad Walker wrote:
Nikki O'Neill wrote:Paul:
Another technique you might want to consider is casting bllets in a box mold, creating a reverse felief. You would make a positive relief element in plaster and cast over it in a box. The method was taught and demonstratd by Ted Sawyer from Bullseye, and they now have a new TipSheet (#5) on the method. You can download the tipsheet from their site. The pieces done in our class using BE casting billets came out amazingly clear and needed little if any cold working. A key element is the use of a refractory wall mold made by screwing pieces of Skamol compressed vermiculite together. The mold is re-usable. A really interesting technique.
Bullseye is doing a demo on this at the upcoming Warm Glass Weekend conference.
They are also going to show this technique at our next Portland chapter meeting of the Oregon Glass Guild.

Jim
Lauri Levanto
Posts: 270
Joined: Tue Mar 11, 2003 7:33 am
Location: Halikko, Finland

Post by Lauri Levanto »

Negative relief casting is easy and interesting.
The front surface is clear, it is the air surface
in the mold. The figure is in the rear surface and
has the (un)smoothness of the mold surface.

One interesting observation was that when I
casted a _positive_ relief of rounded female form.
It seems positive from both sides,
that is, seen from air and mod side.

The same with a sailboat behaved differently.
A sailboat (with sharp lines and large curved areas)
looks fine (in negative relief) fron the air side,
but looks negative -like the hull carved in water-
when seen from the mold side.

-lauri
PDXBarbara
Posts: 292
Joined: Sun Mar 09, 2003 4:09 pm
Location: Portland, OR

Post by PDXBarbara »

jim simmons wrote:
They are also going to show this technique at our next Portland chapter meeting of the Oregon Glass Guild.

Jim
PDX chapter meeting: last Wednesday of September.
BB
Barbara Bader