Where can I buy Cerium Oxide

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Val
Posts: 35
Joined: Sun May 25, 2003 8:01 pm
Contact:

Where can I buy Cerium Oxide

Post by Val »

Does anybody know where I can buy cerium oxide in Ontario?

Val
Lonman
Posts: 17
Joined: Mon Jun 09, 2003 11:37 pm
Location: Ennis, Texas
Contact:

Where can I buy cerium oxide?

Post by Lonman »

A & A Products in Texas
They are on the Warm Glass links.

8)
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Where can I buy Cerium Oxide

Post by Bert Weiss »

Val wrote:Does anybody know where I can buy cerium oxide in Ontario?

Val
CR Laurence (905) 303-7966
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Val
Posts: 35
Joined: Sun May 25, 2003 8:01 pm
Contact:

Post by Val »

Thanks for the info.

Val
Allan Gott
Posts: 19
Joined: Mon Mar 10, 2003 11:57 am
Location: Calgary
Contact:

Post by Allan Gott »

Call Terry Craig at the Living Arts Center in Mississauga Val. He'll know the best source in S. Ontario.
Carolyn Ledbetter
Posts: 17
Joined: Mon Mar 10, 2003 1:29 pm
Location: Venice, Florida

Post by Carolyn Ledbetter »

Val,
Just a thought - Do you have a rock (gem and mineral type) shop nearby? They usually carry abrasives and polishing compounds including cerium oxide.