Cliff
Drilling out a bubble
Moderators: Brad Walker, Tony Smith
-
Cliff Swanson
- Posts: 65
- Joined: Sun Mar 09, 2003 10:36 pm
- Location: Raleigh, NC
Drilling out a bubble
I'm working on eliminating surface distortion due to a bubble. I've just drilled into the bubble, but have not drilled all the way through the full 6 mm thickness, just into the bubble, so it now appears like a crater on a volcano
. Is it necessary to drill completely through the full thickness of the blank, or is simply opening up a hole sufficient before laying in some frit and firing to full fuse to mend the defect?
Cliff
Cliff
-
Terry Ow-Wing
- Posts: 124
- Joined: Sun Mar 09, 2003 3:21 pm
- Location: San Francisco, Ca.
- Contact: