What is a good mesh size for sifting Bullseye fine powdered frits. Has anyone used the sifting cloth that Schlaifers carries.
Is the stainless screen any better? Secrets of an even dense to light color blend?
Sifters for powdered frits
Moderators: Brad Walker, Tony Smith
-
Joseph Tracy
- Posts: 33
- Joined: Thu Mar 13, 2003 5:08 pm
- Location: Stamford, Vermont
- Contact:
-
Brad Walker
- Site Admin
- Posts: 1544
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Bullseye's fine frit is 0.2 to 1.2 mm. That's around 20 mesh, which is larger than any of the sifters that Schlaifer's carries (by the way, most of what they carry is made by Thompson Enamel).
Bullseye powder is around 80 mesh, so you can use any of the 80 mesh sifters to sift the powder. (These work with Uroboros/System 96 powder also.) The screens work fine for me, but there's no reason why the cloth wouldn't work just as well. And, as Brock mentions, a tea strainer works, too (and it's usually cheaper and better made).
Bullseye's tip sheet #4 has some good tips on how to get a dense to light color blend. They suggest sifting a layer over the entire area, then sifting again over 3/4 of the area, then 1/2, then the final 1/4. (I break the area into more than 4 parts, but you get the idea.) A light box will help you make sure it's even.
You can download the tip sheet (as well as several others) from this page: http://www.bullseyeconnection.com/getsmart.html
Bullseye powder is around 80 mesh, so you can use any of the 80 mesh sifters to sift the powder. (These work with Uroboros/System 96 powder also.) The screens work fine for me, but there's no reason why the cloth wouldn't work just as well. And, as Brock mentions, a tea strainer works, too (and it's usually cheaper and better made).
Bullseye's tip sheet #4 has some good tips on how to get a dense to light color blend. They suggest sifting a layer over the entire area, then sifting again over 3/4 of the area, then 1/2, then the final 1/4. (I break the area into more than 4 parts, but you get the idea.) A light box will help you make sure it's even.
You can download the tip sheet (as well as several others) from this page: http://www.bullseyeconnection.com/getsmart.html
-
Joseph Tracy
- Posts: 33
- Joined: Thu Mar 13, 2003 5:08 pm
- Location: Stamford, Vermont
- Contact: