I need to remove liver of sulfur patina on silver foil. Can someone tell me at what temps. it will burn off.
Thanks ...K
-
Brock
- Posts: 1519
- Joined: Mon Mar 10, 2003 1:32 pm
- Location: Vancouver, B.C.
Post
by Brock »
By 1000f
My memory is so good, I can't remember the last time I forgot something . . .
-
KellyG
- Posts: 67
- Joined: Sun Mar 09, 2003 11:12 pm
- Location: Baton Rouge, LA
-
Contact:
Post
by KellyG »
Thanks Brock. It was 850 in my kiln. Your answer surprised me tho. I thought it would have been below 500. Glad I posted and you answered.
...K