Well . . . it should work 4 times as quickly. BrockTony Smith wrote:So, do you think 1200F was too hot?Brock wrote:. . . You know me... forever the experimentalist... gotta try EVERYTHING. Next, I'm going to see if I can slump plastic. Hmmmmm . . .
You can. A friend of mine slumps small plexiglass mock-ups of larger glass sculptures. Approx. 300F in your stove. Brock
Spectrum Silvercoats Fusing Experiment
Moderators: Brad Walker, Tony Smith
My memory is so good, I can't remember the last time I forgot something . . .
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
it would be so bad of me to keep going with this....
I've been slumping acrylic for at least 20 years in the oven... I guess I should have made that more obvious... but it does explain the strange taste in the meatloaf.
Tony
I've been slumping acrylic for at least 20 years in the oven... I guess I should have made that more obvious... but it does explain the strange taste in the meatloaf.
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact: