I have been hunting around for info on the technique and so far haven't found a thing. So.... What is going on when people laminate glass as in the work by James Shaw and Steve Ledterman? Is the glass fused together or are they gluing things together like some optical lenses?
Thanks and hiyas!
Karl
Laminated Glass?
Moderators: Brad Walker, Tony Smith
-
Ron Coleman
- Posts: 468
- Joined: Sun Mar 09, 2003 3:20 pm
- Location: Columbus, Ohio USA
http://ips.addr.com/artist_pages/ledterman/
http://ips.addr.com/artist_pages/shaw/
Glued with special optically clear adhesive and hours of cold working.
Ron
http://ips.addr.com/artist_pages/shaw/
Glued with special optically clear adhesive and hours of cold working.
Ron
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Laminated Glass?
Hxtal epoxy. $1000 per gallon at HIS glassworks. That was the price, last I knew, a few years ago.K Boggs wrote:I have been hunting around for info on the technique and so far haven't found a thing. So.... What is going on when people laminate glass as in the work by James Shaw and Steve Ledterman? Is the glass fused together or are they gluing things together like some optical lenses?
Thanks and hiyas!
Karl
Bert
Bert Weiss Art Glass*
http://www.customartglass.com