What is a good mesh size for evenly sifting bullseye powder frits?
Has anyone used non traditional sifters with good results?
Sifting screens for powdered frits
Moderators: Brad Walker, Tony Smith
-
Joseph Tracy
- Posts: 33
- Joined: Thu Mar 13, 2003 5:08 pm
- Location: Stamford, Vermont
- Contact:
-
Ron Coleman
- Posts: 468
- Joined: Sun Mar 09, 2003 3:20 pm
- Location: Columbus, Ohio USA
I use the three small sifters shown at the top of this page on Thompson Enamels site. These sifters are plastic with metal mesh and wire handles.
http://thompsonenamel.com/products/tools/grinding.htm
They are 40 mesh and all BE powders will go through them and they don't drip powder. You have to tap gently to get the powders to feed.
Ron
http://thompsonenamel.com/products/tools/grinding.htm
They are 40 mesh and all BE powders will go through them and they don't drip powder. You have to tap gently to get the powders to feed.
Ron
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
RonRon Coleman wrote:I use the three small sifters shown at the top of this page on Thompson Enamels site. These sifters are plastic with metal mesh and wire handles.
http://thompsonenamel.com/products/tools/grinding.htm
They are 40 mesh and all BE powders will go through them and they don't drip powder. You have to tap gently to get the powders to feed.
Ron
Running your finger nails up and down the twisted wire handles works well to get the frits to come out.
Bert
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
[quote="Ron Coleman"]I use the three small sifters shown at the top of this page on Thompson Enamels site. These sifters are plastic with metal mesh and wire handles.
http://thompsonenamel.com/products/tools/grinding.htm
Was looking at this site to see the sifters. They also offer screens and screen materials in a variety of "mesh sizes" for separating frit sizes. Is there a conversion chart somewhere that gives the opening size in these meshes in either inches or metric measurements? It would be useful to know which to order for separating homemade frit.
Thanks.
C.
http://thompsonenamel.com/products/tools/grinding.htm
Was looking at this site to see the sifters. They also offer screens and screen materials in a variety of "mesh sizes" for separating frit sizes. Is there a conversion chart somewhere that gives the opening size in these meshes in either inches or metric measurements? It would be useful to know which to order for separating homemade frit.
Thanks.
C.
-
Ron Coleman
- Posts: 468
- Joined: Sun Mar 09, 2003 3:20 pm
- Location: Columbus, Ohio USA
Try this site CarolCarol wrote:Ron Coleman wrote:I use the three small sifters shown at the top of this page on Thompson Enamels site. These sifters are plastic with metal mesh and wire handles.
http://thompsonenamel.com/products/tools/grinding.htm
Was looking at this site to see the sifters. They also offer screens and screen materials in a variety of "mesh sizes" for separating frit sizes. Is there a conversion chart somewhere that gives the opening size in these meshes in either inches or metric measurements? It would be useful to know which to order for separating homemade frit.
Thanks.
C.
http://www.processassociates.com/proces ... sieves.htm
Ron