Capping blasted irid
Moderators: Brad Walker, Tony Smith
-
DonMcClennen
- Posts: 381
- Joined: Sun Mar 09, 2003 9:09 pm
- Location: Ontario
Capping blasted irid
After sanblasting a design on "96" black irid, do I need to fire polish before I clear cap? or can I clear cap (about 14" dia.) over the blasted design and get good result?
"The Glassman"
-
DonMcClennen
- Posts: 381
- Joined: Sun Mar 09, 2003 9:09 pm
- Location: Ontario
-
artquestor
- Posts: 4
- Joined: Sat Apr 26, 2003 11:52 pm
- Location: Northern California
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Clear cap means to cap with clear, or to cover the piece with clear glass and fuse it together.artquestor wrote:Just curious, what does "clear cap" mean? (ignorant of sandblasting)
Susanne
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun