Hi All,
I am using a new slumping mold - a bowl with ruffled edges, but is deeper than the molds I usually use. The diameter of this slumping mold is 11 1/2" when using a ruler across the top. The diameter using a soft measuring tape across the diameter and down into the bowl is 13".
I want as big a bowl as possible, but I'm worried about using a 13" fused disc for this mold, since the overhang would be over an inch. Has anyone figured this one out already? How big a fused disc can I use?
Thanks in advance,
Pat Loboda
Deep Slumping Mold
Moderators: Brad Walker, Tony Smith
-
Pat Loboda
- Posts: 29
- Joined: Tue Mar 11, 2003 9:00 pm
- Location: Bay City, Michigan
- Contact:
-
Joanne Owsley
- Posts: 52
- Joined: Wed Apr 16, 2003 4:27 pm
- Location: Arlington, WA
- Contact:
Could you, perhaps, slump it slightly in something larger and more shallow and THEN put it in your new mold for a second slump? It seems that if you get it to drop in the middle a little, the sides would pull in and not over hang your new mold so much.
Just a thought.
Just a thought.
~ Joanne
"What neglected medication made you think THAT was a good idea??"
- me, to myself
"What neglected medication made you think THAT was a good idea??"
- me, to myself
-