glass paints

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
ellen abbott
Posts: 148
Joined: Tue Mar 11, 2003 12:04 pm
Location: Houston Tx
Contact:

glass paints

Post by ellen abbott »

Can anyone recommend a type of glass paint that fires at less than the softening point for Bullseye?

E
Brad Walker
Site Admin
Posts: 1537
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Post by Brad Walker »

Do you mean softening point (1250 for Bullseye transparents, 1270 for opals), or do you mean the point at which the glass starts to deform in the heat?

If you really mean softening point, than we can probably come up with some paints that mature at below 1250 (especially opaque paints). For example, Paradise Paints will adhere at 1150, but you'll get a matt finish.

If you mean when the glass deforms, that's harder, at least if you want a paint that will be permanent, rather than just brushed or sprayed on a (usually sandblasted) surface.
ellen abbott
Posts: 148
Joined: Tue Mar 11, 2003 12:04 pm
Location: Houston Tx
Contact:

Post by ellen abbott »

It's a cast piece (one of my cup forms) that I mis-judged on the amount of bronze color and the whole thing came out very brown. Too brown. What I want to do is use paints to give it more color without deforming the cast piece, and I would like the paints to be permanent so I figured they would have to be fired on.

e
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Post by Brock »

ellen abbott wrote:It's a cast piece (one of my cup forms) that I mis-judged on the amount of bronze color and the whole thing came out very brown. Too brown. What I want to do is use paints to give it more color without deforming the cast piece, and I would like the paints to be permanent so I figured they would have to be fired on.

e
Low fire enamels.

C'est pas moi sac, but aren't there enamels that fire as low as 950?

Brock
My memory is so good, I can't remember the last time I forgot something . . .
Brad Walker
Site Admin
Posts: 1537
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Post by Brad Walker »

Brock wrote: C'est pas moi sac, but aren't there enamels that fire as low as 950?
Don't know of any, though they could be out there. Maybe in France (or is that Quebec?).

Thompson doesn't have any, FuseMaster doesn't have any, Paradise Paints don't do it, neither does the stuff from Ferro.

Traditional stained glass colors mature too high (Reusche is 1250 to 1400, but Elskus says they work at 1100 to 1250, Drakenfield is 1050 to 1080, but Elskus says a few work at a lower temp). Silver stain might work, since it matures at 950 to 1050, but I'm not sure if that limited color range will work for Ellen (or if she wants to tackle that learning curve).
Tony Smith
Posts: 1037
Joined: Sun Mar 09, 2003 5:59 pm
Location: Massachusetts, USA
Contact:

Post by Tony Smith »

There's the entire Pebeo line that fire at 300°, but I don't have any experience with them. I believe they are available at Michael's or AC Moore.

I suggest an experiment first.

http://www.dickblick.com/zz029/08/products.asp?param=0

and

http://www.dickblick.com/zz029/50/produ ... ig_id=3689

Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
ellen abbott
Posts: 148
Joined: Tue Mar 11, 2003 12:04 pm
Location: Houston Tx
Contact:

Post by ellen abbott »

Thanks Tony (and Brad and Brock). I'll check them out.

e
Brad Walker
Site Admin
Posts: 1537
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Post by Brad Walker »

Paints like the Pebeo ones are heated (usually in a kitchen oven) to 325F. They go on brilliant and look great at first, but after a few years they dull and often crack off.

Most "glass painting" books are done with paints like these in mind. The significant exception is Albinus Elskus's The Art of Painting on Glass, which is the classic text for traditional stained glass painting.
Rebecca M.
Posts: 126
Joined: Fri Sep 12, 2003 12:15 pm
Location: Myrtle Beach
Contact:

Post by Rebecca M. »

I haven't tried these yet, but it has a pretty low firing point for glass paints.
http://www.mrandmrsofdallas.com/Product ... Paints.htm

Some of the ices if you can find them can be fired pretty low, but will be raised in a granular texture. Also would need to be horizontal, so they might not help. I don't know where you'd get them anyway. Thompson supposedly has a line of low-fire ices, but?????

And I've heard, but again haven't tried Reushe products "D" and "MB" can mature at 1100 with a 15 min. hold.
Ian
Posts: 30
Joined: Fri Sep 12, 2003 2:44 pm
Location: Amalinda, South Africa

Post by Ian »

Hi
I have been trying Vidtriate's products for a while now and find them very good. They have a range of low fusing paints for glassware at 500 to 600C ( 932 to 1112F) see http://www.vidriarte.com/colores-fritas/pint-baja.htm Haven't tried these yet but if they are like their products for float then they will be good.
Regards
Ian
jerry flanary
Posts: 158
Joined: Tue Sep 09, 2003 11:11 pm
Location: norfolk, va

Post by jerry flanary »

I mis-judged on the amount of bronze color and the whole thing came out very brown. Too brown. What I want to do is use paints to give it more color without deforming the cast
Was it a bronze powder? Does it now have a layer of bronze on the outside? If so, why not Patena?
j.

A lack of doubt doesn't lend certainty.
ellen abbott
Posts: 148
Joined: Tue Mar 11, 2003 12:04 pm
Location: Houston Tx
Contact:

Post by ellen abbott »

It was frit size 1 BE lt. bronze glass (don't have the # in my head). I should have cut it with clear (50/50), which I forgot to do and I should have used less. Only wanted the cup itself to be brown (it has branch forms on the outside like a bird's nest) and the foot to be clear. Well, not clear since the clear #1 frit becomes very cloudy. Mis-judged the quantity of bronze so it over-powered the clear for the foot and it all came out brown. My intention is to paint green leaves on the foot to give it some contrast. All that aside, what do you mean by 'Patena' (as in a brand name or patina)?

E
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: glass paints

Post by Bert Weiss »

ellen abbott wrote:Can anyone recommend a type of glass paint that fires at less than the softening point for Bullseye?

E
Ellen

You have many choices. There are lots of enamels that are designed to be fired in around 1050ºF. The idea is that they can be applied to glassware and not slump it. Colors come in transparent and opaque as well as precious metals and lustres. I would probably suggest working with colors from Reusche. Fusemaster might have a good line of low fires, I forget exactly. There are some other sources. The good transparent colors from Germany are more difficult to get here in the US.

If you choose to use the really low fire organic colors, I suggest working with Ferro Organic Bottle Coatings. They fire in at 400ºF for 1/2 hour and come in brilliant transparent colors.

The difference between the 2 lines of colors is that the 1050ºF colors will scratch with a knife. The 400ºF colors can be razor bladed off with lots of effort. Both lines of color will hold up to repeated dishwashing.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Tom White
Posts: 174
Joined: Tue Mar 11, 2003 9:14 am
Location: Houston, Texas

Post by Tom White »

Ellen, I think that Jerry was suggesting that if the piece had actual bronze metal on the surface you could use one of the many available solutions to patina the metal surface to the green or blue color of weathered bronze. Since you have no metal on your cup this suggestion would not work for you.
The glass colors from Mr & Mrs of Dallas are used for painting on thin milkglass lamp shades so they do mature at low temps to avoid distorting such thin glass shapes. They are available in very small quantities, suitable for individual painters.

Best wishes,
Tom in Texas
Post Reply