Firing glass for jewelry....

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Joanne in QB
Posts: 3
Joined: Tue Sep 30, 2003 10:14 pm
Location: Qualicum Beach, BC

Firing glass for jewelry....

Post by Joanne in QB »

I have read in GPQ that you can fire small pieces - to 2 inches across - at 1475 degrees per hour (to 1475 degrees) - that seems awfully fast. Any comments or advise?
Tom White
Posts: 174
Joined: Tue Mar 11, 2003 9:14 am
Location: Houston, Texas

Post by Tom White »

In my small (6"x6"x6") quickfire tabletop fiber kiln it is hard to fire slower. I use pieces of 1 1/2" square regularly to test new colors or ideas. My larger ceramic kilns will not fire that fast.

Best wishes,
Tom in Texas
Paul Tarlow
Posts: 344
Joined: Sun Mar 09, 2003 4:06 pm
Location: Helios Kiln Glass Studio - Austin
Contact:

Re: Firing glass for jewelry....

Post by Paul Tarlow »

Joanne in QB wrote:I have read in GPQ that you can fire small pieces - to 2 inches across - at 1475 degrees per hour (to 1475 degrees) - that seems awfully fast. Any comments or advise?
Most kilns cannot heat up fast enough to thermal shock small (jewelry sized) pieces of glass. Likewise, most kiln naturally cool slowly enough to properly anneal small peices of glass.

One thing to beware of with very rapid heating or cooling is that it is possible to thermal shock a kiln shelf.

- Paul
Joanne in QB
Posts: 3
Joined: Tue Sep 30, 2003 10:14 pm
Location: Qualicum Beach, BC

Thanks

Post by Joanne in QB »

for the input - also thanks for the comment on the kiln shelf - a very good reason not to heat small pieces as fast as you can in a larger kiln.
Tim Swann
Posts: 83
Joined: Mon Mar 10, 2003 9:47 pm
Location: San Diego, CA

Post by Tim Swann »

I have a small 8"x8"x8" kiln the has only one firing ramp "Fast". It gets to 1500°F within 60 minutes. The cool down time is about the same as a large kiln. It will give me about 3 hours between 1100°F and 900°F. The largest component I have made in this kiln is 3"x5"x1/4". I seldom have any problems with either the ramp up or ramp down. My size limiyt is caused more by the way the elemnet heats the kiln (U shaped element, front load kiln, no elementon the door).

Tim
Dani
Posts: 493
Joined: Mon Mar 10, 2003 3:17 pm
Contact:

Post by Dani »

Can you use a phaser to slow down the ramping on those itty bitty kilns?
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Post by Brock »

Dani wrote:Can you use a phaser to slow down the ramping on those itty bitty kilns?
Nah, phasers only work on Klingons, you want a rheostat. Brock
My memory is so good, I can't remember the last time I forgot something . . .
Tom White
Posts: 174
Joined: Tue Mar 11, 2003 9:14 am
Location: Houston, Texas

Post by Tom White »

I have mounted a 120 volt bi-metal infinite switch and a regular duplex 120 volt outlet in a deep square electrical box with a 6' cord to plug into the wall outlet. The kiln plugs into the controlled outlet and this allows me to slow the rate of rise somewhat. Paragon sells the equivalent with the switch mounted in a smaller box about 12 to 18" from the outlet end of a heavy duty extension cord. I start the kiln with the switch at the lowest position which provides current to the kiln and place a kiln post on its side under the front edge of the kiln muffle to vent it and slow the rate of heating until the pyrometer indicates 1000 F. I never have to set the switch any hotter than medium, even when I do my mini pot melts in that kiln.

Best wishes,
Tom in Texas
Tim Swann
Posts: 83
Joined: Mon Mar 10, 2003 9:47 pm
Location: San Diego, CA

Post by Tim Swann »

When I want to slow down the small kiln I have I do it by turning it off and on. It may seem crud but I only need to do this when I am doing a second fusing or batch annealing beads. I have considered putting a rheostat in line with the plug, but have not found it to be necessary yet.

Tim
vidrio
Posts: 21
Joined: Thu Sep 04, 2003 7:14 pm

Post by vidrio »

Brock wrote:
Dani wrote:Can you use a phaser to slow down the ramping on those itty bitty kilns?
Nah, phasers only work on Klingons, you want a rheostat. Brock
Hi Brock,

I'm new to pendent making, new to glass really. I've been playing with temps to try and get the right shapes. If I cut squares they with take on circular shapes at 1550, but they get very fat. 1480 seems to underfire them. Any suggestions. Also, if you have any basic info on what prefired cut shapes become when fired it would help. I've tried a lot of different tests and still don't seem to have any consistent answers. I've also been trying to get holes with fiber paper, with no luck. I'm tring to find some bead release as I understand that works with toothpicks, but do you know anything different?

Thanks Vidrio
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Post by Brock »

Hi Brock,

I'm new to pendent making, new to glass really. I've been playing with temps to try and get the right shapes. If I cut squares they with take on circular shapes at 1550, but they get very fat. 1480 seems to underfire them. Any suggestions. Also, if you have any basic info on what prefired cut shapes become when fired it would help. I've tried a lot of different tests and still don't seem to have any consistent answers. I've also been trying to get holes with fiber paper, with no luck. I'm tring to find some bead release as I understand that works with toothpicks, but do you know anything different?

Thanks Vidrio

I'm a big fan of LOOKING in the kiln so I know exactly what shape I have achieved. Basically, glass will soften, move, and try to round, so with enough heat, square become circles, rectangles become lozenges, etc. Of course, any of these processes/shapes can be halted at any time by LOOKING in the kiln and stopping it where tyou want. I have zero experience with bead/pendant holes but lots of people here do. Brock
My memory is so good, I can't remember the last time I forgot something . . .
Barbara Muth
Posts: 382
Joined: Sun Mar 09, 2003 8:10 pm
Location: Washington DC Metropolitan Area
Contact:

Post by Barbara Muth »

Vidrio, try using fiber paper , or bead release coated steel mandrels for bead holes. Some folks have had less than success with bead release coated toothpicks.

if you are new to glass I strongly recommend that you purchase the "bible" Brad's Warmglass book. When I was learning about glass and just started fusing I worked with a tabletop kiln, a little Paragon Quickfire with a 4 inch shelf. I read Brad's book, read the board, experimented and did a lot of peeking in the kiln. (I heartily agree with Brock - if you want to really control, until you run a lot of tests peeking is the answer, particularly when you do not have a digital controller)

You can order Brad's book from this website, the link is on the top of the page to the right.

Have fun!
barbara
Barbara
Check out the glass manufacturer's recommended firing schedules...
LATEST GLASS
jim simmons
Posts: 478
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Post by jim simmons »

Barbara Muth wrote: When I was learning about glass and just started fusing I worked with a tabletop kiln, a little Paragon Quickfire with a 4 inch shelf.
barbara
You astound me, Barbara. Here I thought that I was the only one left in the world that had one of those little 4" jobs. :wink:

Jim
JoanB
Posts: 4
Joined: Mon Mar 10, 2003 6:10 pm

Post by JoanB »

I only make fused glass jewelry. I frequently ramp the kiln at 1500 per hour, with no problems at all, to either the glass or the shelf.
After soaking at the appropriate temp, I crash cool the kiln to about 1050, and simply close the kiln and let it cool to room temp. I've been doing this for over five years, and have never had any problem with any of my pieces.

My first kiln was the Paragon Quik-Fire, but mine came with a 5" X 5" shelf. I did use the Paragon 'temperature controller' (which is actually a rheostat) and got pretty good in getting predictable results.

I now use a Paragon SC-2 which comes with a digital controller. Once you've had the luxury of the digital controller, there's just no going back! It's only a little larger... uses a 7" X 7" shelf, but it works for my needs.

JoanB
Barbara Muth
Posts: 382
Joined: Sun Mar 09, 2003 8:10 pm
Location: Washington DC Metropolitan Area
Contact:

Post by Barbara Muth »

jim simmons wrote:
Barbara Muth wrote: When I was learning about glass and just started fusing I worked with a tabletop kiln, a little Paragon Quickfire with a 4 inch shelf.
barbara
You astound me, Barbara. Here I thought that I was the only one left in the world that had one of those little 4" jobs. :wink:

Jim
Jim, I keep thinking I will use it as a test kiln so I don't sell the Marshmallow... But I haven't used it in a year and a half, not since I fired up my Jennie. I did learn a lot from the Marshmallow though, and I do think it is a good way to get your feet wet!

Barbara
Barbara
Check out the glass manufacturer's recommended firing schedules...
LATEST GLASS
Bea
Posts: 23
Joined: Tue Aug 05, 2003 8:53 am
Location: Kangaroo Island, South Australia

Post by Bea »

Joan

"After soaking at the appropriate temp, I crash cool the kiln to about 1050, and simply close the kiln and let it cool to room temp. I've been doing this for over five years, and have never had any problem with any of my pieces."

Do you anneal your beads after this????

My first couple of batches using this schedule had a couple of pendants that cracked after some time....... now I crash cool the kiln to 1000F and then let the kiln take over to bring it down to 965F and soak for 30 - 45 mins and so far those pieces have stood the test of time (only a few months at this stage).

I am using the Sierra PMC kiln.......

Bea
Simply Bea Beads
vidrio
Posts: 21
Joined: Thu Sep 04, 2003 7:14 pm

jewelry

Post by vidrio »

Hi, thanks for reply.

A couple more questions.

My kiln will fire at 999 per hour. Once I've got it up to 1500, how long do I need to soak the pieces?

Also, could you give me any advice on attaching findings. I've tried to stay away from adding anything to the glass, not so much as I'm a purist, but more because I'm messy! But, I've had no luck getting holes, or "tunnels in the glass.

Thanks

Vidrio.
JoanB wrote:I only make fused glass jewelry. I frequently ramp the kiln at 1500 per hour, with no problems at all, to either the glass or the shelf.
After soaking at the appropriate temp, I crash cool the kiln to about 1050, and simply close the kiln and let it cool to room temp. I've been doing this for over five years, and have never had any problem with any of my pieces.

My first kiln was the Paragon Quik-Fire, but mine came with a 5" X 5" shelf. I did use the Paragon 'temperature controller' (which is actually a rheostat) and got pretty good in getting predictable results.

I now use a Paragon SC-2 which comes with a digital controller. Once you've had the luxury of the digital controller, there's just no going back! It's only a little larger... uses a 7" X 7" shelf, but it works for my needs.

JoanB
vidrio
Posts: 21
Joined: Thu Sep 04, 2003 7:14 pm

pendents and findings

Post by vidrio »

Thanks for advice,

I guess I've been a little nervous about peeking in the kiln. It seems so HOT! Also, I was told it could ruin glass if you don't know what you're doing. But probably that pertains to bigger pieces. So, I'm going to give it a go.

How do you attach your pendents if you don't use holes? Glues and findings?

Vidrio
Brock wrote:Hi Brock,

I'm new to pendent making, new to glass really. I've been playing with temps to try and get the right shapes. If I cut squares they with take on circular shapes at 1550, but they get very fat. 1480 seems to underfire them. Any suggestions. Also, if you have any basic info on what prefired cut shapes become when fired it would help. I've tried a lot of different tests and still don't seem to have any consistent answers. I've also been trying to get holes with fiber paper, with no luck. I'm tring to find some bead release as I understand that works with toothpicks, but do you know anything different?

Thanks Vidrio

I'm a big fan of LOOKING in the kiln so I know exactly what shape I have achieved. Basically, glass will soften, move, and try to round, so with enough heat, square become circles, rectangles become lozenges, etc. Of course, any of these processes/shapes can be halted at any time by LOOKING in the kiln and stopping it where tyou want. I have zero experience with bead/pendant holes but lots of people here do. Brock
Dolores
Posts: 106
Joined: Mon Jul 14, 2003 9:21 pm
Location: Sunny Southern California
Contact:

Post by Dolores »

Just some possibilities for hanging pendants:
-drill a small hole for a jumpring.
-drill small holes on opposite corners and attach jumprings and chain.
-glue on a pendant bail (lots of sources to be found in the archives!).
-grind a channel all around the glass and wire wrap.
-glue on a PMC backing or cut a custom shape out of sheet metal.

In regards to the pendant channels, be sure to overlap the top layer over the fiber paper enough to allow the glass to sag over (if not, it will retreat back instead). One good trick is to close the opening with a ceramic rod once the glass has softened. I got tired of wasting firings on channels that didn't want to close properly, so I donned a kiln glove and pushed the offending glass down with the ceramic firing rod (Voile! Nice closed channels every time! :D ). Yes, the kiln is at 1400 degrees at this point, but small jewelry pieces are not affected.

DOLORES
Jack Bowman
Posts: 127
Joined: Mon Mar 17, 2003 10:52 pm
Location: Utah
Contact:

Re: jewelry

Post by Jack Bowman »

[quote="vidrio"]Hi, thanks for reply.

A couple more questions.

My kiln will fire at 999 per hour. Once I've got it up to 1500, how long do I need to soak the pieces?

Also, could you give me any advice on attaching findings. I've tried to stay away from adding anything to the glass, not so much as I'm a purist, but more because I'm messy! But, I've had no luck getting holes, or "tunnels in the glass.

Thanks

Vidrio.

This company sells a great bail. Just glue on with E6000

http://www.stainedglasswarehouse.com/jewelrybails.html

Jack
Post Reply