rose
Posts: 1
Joined: Sun Oct 12, 2003 8:43 pm

firing wine bottles cone#

Post by rose »

need to know what cone to use to fire wine bottles in a ceramic kiln if anyone has use a ceramic kiln and knows what cone share it please
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Post by Brad Walker »

Around cone 017, sometimes 016.

You may have to experiment a bit, but that's usually in the right area.