Here is a picture of yesterdays pot melt experiment. (The small disk is the bottom of the flo
I also got a few bubbles, the largest being 1/4".
http://users.wi.net/~magnum/Melt/CloseUp.JPG
They popped and have very sharp edges. What would be the best way to deal with them. Should I put the piece back in and cook them out? Or fill them with clear frit and re-fire?
Here are some interesting facts. I started out with 3.4 pounds of glass. It made a 12-1/2" (almost round) diameter piece that weighs an even 3 pounds. I weighed the pot before and after and the remaining 4 ounces of glass is now permenently part of the pot. I applied 12 coats of kiln wash and all 12 layers stuck to the bottom of the piece but luckly came off with the help of an S.O.S. pad and some elbow grease.
Randy