I need some help in knowing how to get the effect on the glass from this WEB page http://www.alchemy-glass.com , they build glass sinks and they use frit encased between 2 layers of glass.
Thanks for your help
Israel Zonzinski
gmusical@racsa.co.cr
From Costa Rica
Effect on glass
Moderators: Brad Walker, Tony Smith
-
Steve Immerman
- Posts: 208
- Joined: Sun Mar 09, 2003 4:55 pm
- Location: Eau Claire, Wisconsin
- Contact:
Oxides
This was discussed a while ago in this thread:
http://www.warmglass.com/cgi-bin/wgarch ... read=71010
Steve
http://www.warmglass.com/cgi-bin/wgarch ... read=71010
Steve
Read that discussion now before posting this reply, and I see something that might be incorrect in the discussion: I don't think Alchemy Glass sinks are 2 inches thick.
Last fall I was commissioned to build a sink and my research lead me to the Alchemy Glass web site and to a showroom in Bethesda, MD where Alchemy shows its sinks. Of the dozen or so pieces on display all were in the 3/4 inch to 1 inch range. I also saw that in addition the the oxides and minerals fused between layers of glass, there were intricate copper inclusions of leaf and (I think) fossil forms. The copper was acid-etched to create an effect of a partially decomposed leaf. Really beautiful stuff.
Check out my finished sink bowl in the photos board, the posting by "lohman". I have a few pics documenting the firing if anyone is interested.
Last fall I was commissioned to build a sink and my research lead me to the Alchemy Glass web site and to a showroom in Bethesda, MD where Alchemy shows its sinks. Of the dozen or so pieces on display all were in the 3/4 inch to 1 inch range. I also saw that in addition the the oxides and minerals fused between layers of glass, there were intricate copper inclusions of leaf and (I think) fossil forms. The copper was acid-etched to create an effect of a partially decomposed leaf. Really beautiful stuff.
Check out my finished sink bowl in the photos board, the posting by "lohman". I have a few pics documenting the firing if anyone is interested.
Last edited by lohman on Wed Mar 26, 2003 12:54 am, edited 1 time in total.
-