This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.
Moderators: Brad Walker , Tony Smith
Mlynn
Posts: 3 Joined: Sat Apr 19, 2003 7:28 pm
Location: Chapel Hill, NC
Contact:
Post
by Mlynn » Thu Oct 23, 2003 11:02 pm
In the threads about fiber paper there's been a lot of discussion about pre-firing. I al so know that folks say it's not needed with thin-fire - but many times I get scuz on the edges of pieces with thin fire underneath. Woukd prefiring prevent this? (Or will thin fire crumble under prefiring?)
Brad Walker
Site Admin
Posts: 1524 Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:
Post
by Brad Walker » Thu Oct 23, 2003 11:39 pm
Thin fire can fall apart with pre-firing.
The new thin fire is supposed to be less likely to scuz the edges than the old.
Brock
Posts: 1519 Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.
Post
by Brock » Thu Oct 23, 2003 11:43 pm
Brad Walker wrote: Thin fire can fall apart with pre-firing.
The new thin fire is supposed to be less likely to scuz the edges than the old.
But then, kiln wash doesn't scuz the edges at all. Imagine that! Brock
My memory is so good, I can't remember the last time I forgot something . . .
Brad Walker
Site Admin
Posts: 1524 Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:
Post
by Brad Walker » Thu Oct 23, 2003 11:47 pm
Brock wrote: Brad Walker wrote: Thin fire can fall apart with pre-firing.
The new thin fire is supposed to be less likely to scuz the edges than the old.
But then, kiln wash doesn't scuz the edges at all. Imagine that! Brock
No pre-firing, either!
Peg
Posts: 74 Joined: Tue Apr 08, 2003 7:50 am
Location: Bristol, UK
Post
by Peg » Fri Oct 24, 2003 7:21 am
Brad Walker wrote: Brock wrote: Brad Walker wrote: Thin fire can fall apart with pre-firing.
The new thin fire is supposed to be less likely to scuz the edges than the old.
But then, kiln wash doesn't scuz the edges at all. Imagine that! Brock
No pre-firing, either!
..apart from the pre-fire needed to dry the shelf, of course.