In the screen printing process you buy blank pre-made screens and add your art work.
There are several different processes for transfering your designs to the screens for printing. Some of the processes are simple, such as directly drawing your designs on the screens and others get more involved, almost like a photographic process. You can use a computer and printer to do it too.
For more information on screen printing see the tutorial below.
http://www.squeegeeville.com/02-screentoday.htm
Ron
There are several different processes for transfering your designs to the screens for printing. Some of the processes are simple, such as directly drawing your designs on the screens and others get more involved, almost like a photographic process. You can use a computer and printer to do it too.
For more information on screen printing see the tutorial below.
http://www.squeegeeville.com/02-screentoday.htm
Ron
Thanks for the link - any source links?
Do you have any links for a source for the screens?
-
Ron Coleman
- Posts: 468
- Joined: Sun Mar 09, 2003 3:20 pm
- Location: Columbus, Ohio USA
Try Pocono Screen. Their wood screens are hard to beat, very heavy and rigid. Lots of other stuff too.
http://poconoscreen.com/