i have been making lots of ornaments lately. i discovered that i can glue them up on wax paper and put them in the kiln still attached to the paper. the wax paper burns off clean. it allows me to glue up a bunch, let them dry, stack them up in a box and fire whenever. got a kiln load of four shelves going now. organicsgirl
-
ruthpowers
- Posts: 30
- Joined: Tue Aug 12, 2003 2:13 pm
- Location: Austin, Texas 78704
Say, would you tell me a little more about your ornaments. How big are they? How much will they retail for? Have you done them in past years? What was popular? Xmas tree shapes? Or more abstract? How are you hanging them? I have made a bunch of Xmas-colored bracelets, but didn't think of ornaments.
Ruth Powers
Glass Silver Dance Dogs
Glass Silver Dance Dogs
-
Patty Gray
- Posts: 70
- Joined: Mon Mar 10, 2003 9:47 pm
- Location: Washington
- Contact:
Hi Rosana,
This is great information to pass onto people that are working with kids too. That way you can transport thier projects intact too. I would assume you are using white glue with this. How about using CMC? or even Klyr-fire as the glue? Have fun and thank you for sharing.
Patty
http://www.pattygray.com
This is great information to pass onto people that are working with kids too. That way you can transport thier projects intact too. I would assume you are using white glue with this. How about using CMC? or even Klyr-fire as the glue? Have fun and thank you for sharing.
Patty
http://www.pattygray.com
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
kiln shelf effects: none . wax paper is almost nothing. the carbon burns out. this would be great for kids projects. yes i use white glue. i am not patient enough for klyrfire as a glue. i have to tilt my shelves to load them. there are three thermocouples in my ceramic kiln. i have glued large glued up projects to the shelf for loading. i trim the paper close for who knows what reason. i just trust the carbon to burn out. rosanna
Rosanna,
Thanks for the great new idea!!
Ruth, I have some photos of ornaments that I came up with for some fusing classes I teach. The photos are in my picture trail "sharing ideas" album. They are pretty popular at the stained glass shop where I work.
Vernelle (another Texan)
http://www.picturetrailcom/vernelle
Thanks for the great new idea!!
Ruth, I have some photos of ornaments that I came up with for some fusing classes I teach. The photos are in my picture trail "sharing ideas" album. They are pretty popular at the stained glass shop where I work.
Vernelle (another Texan)
http://www.picturetrailcom/vernelle
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
I love wax paper when I get a little overzealous with glue. I can just peel it off after it dries and put it in the kiln on a kiln shelf( prepared of course). I am always worried about anything getting on my shelves or elements. I know I won't ever spend that much on a piece of equipment again. My husband would freak.Lia
-
Melissa Terman
- Posts: 52
- Joined: Tue Mar 18, 2003 1:07 am
- Location: New York
- Contact:
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
wax paper and Christmas ornaments
I saw, I think in GPQ, where wax paper is used as a base for constructing snowflakes and glueing them together. The snowflake doesn't stick to the wax paper once the glue has dried. Clear nailpolish was used to glue the pieces together. I tried it, and it didn't leave any residue, plus it dried really quickly. I did vent the kiln till the nail polish burned off. I've also been doing a lot of Christmas ornaments, but I'm not sure about the best way to hang them. I am only using single thickness glass with design elements because I want to make them as simple as possible so I can sell them at a reasonable price. Some of the things I've tried for hanging the ornaments were to fuse some nichrome wire for hangers. This worked well, but I had to use a second layer of glass. Then I tried glueing the hooks on with E6000. This didn't work, I was able to pull the hooks off with little effort. I also tried glueing with silicone glue, and this seemed to work best, but is messy. I've drilled holes in the tops. This also works well but is really time consuming. Does anyone have a better method for applying hangers to single thickness ornaments?
Joan
Joan
-
Tony Serviente
- Posts: 328
- Joined: Thu May 29, 2003 11:48 am
- Location: Ithaca,NY
- Contact:
Make copper wire loops, and embed the split between two pieces of glass. When it fuses, the wire is trapped, the sharp split is safely away from the fish line, and you're done. All you need is a little quarter inch piece to sit on top of the ring. Only drawback is you have to go hot enough for the holding piece of glass to fuse to the base, which is well beyond tack. I've done this over the years with great success. Good luck
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
-
ruthpowers
- Posts: 30
- Joined: Tue Aug 12, 2003 2:13 pm
- Location: Austin, Texas 78704
Re: wax paper and Christmas ornaments
joan wrote:I saw, I think in GPQ, where wax paper is used as a base for constructing snowflakes and glueing them together. The snowflake doesn't stick to the wax paper once the glue has dried. Clear nailpolish was used to glue the pieces together. I tried it, and it didn't leave any residue, plus it dried really quickly. I did vent the kiln till the nail polish burned off. I've also been doing a lot of Christmas ornaments, but I'm not sure about the best way to hang them. I am only using single thickness glass with design elements because I want to make them as simple as possible so I can sell them at a reasonable price. Some of the things I've tried for hanging the ornaments were to fuse some nichrome wire for hangers. This worked well, but I had to use a second layer of glass. Then I tried glueing the hooks on with E6000. This didn't work, I was able to pull the hooks off with little effort. I also tried glueing with silicone glue, and this seemed to work best, but is messy. I've drilled holes in the tops. This also works well but is really time consuming. Does anyone have a better method for applying hangers to single thickness ornaments?
Joan
When I fuse a single layer for sun catchers I cut a small triangle of thin clear and place the wire between the cllear tri..and the piece to be hung.
robertb
robert
-
Tony Serviente
- Posts: 328
- Joined: Thu May 29, 2003 11:48 am
- Location: Ithaca,NY
- Contact: