Post by LynArts »

I want to melt wine/beer bottle in my kiln. Does anyone out there know what cone (temperature) I need to shoot for? I hate the thought of having to watch them every minute. My kiln has a kiln-sitter, but not the new computer one. I did this in a former life but can't remember what temp. was good. Thanks for any help. lyn
charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Post by charlie »

1525 for 10 minutes
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Post by Brad Walker »

Click on Search at the top of the page. Enter bottle into the form. You'll get more information about this subject than you probably wanted.