Anyone know exactly what combination of metals makes up variegated red? I know there's copper in there, but what else?
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: Variegated red

Post by Brock »

Brad Walker wrote:Anyone know exactly what combination of metals makes up variegated red? I know there's copper in there, but what else?
Not a clue! But I wish they made it in foil. I've been working with it all day, and it tears and curls SO much more than foils. Brock
My memory is so good, I can't remember the last time I forgot something . . .
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Post by Brad Walker »

Yeah, I've got a bunch of leaf, it fires a gorgeous blue (now why does something called variegated red fire to blue????)

By the way, I'm also playing with variegated green and variegated black -- they are similar, except less vivid blue and more black. I suspect the black is aluminum, and would imagine there's a little silver in there also. If I could get a recipe from somewhere, I'd try to make something a little thicker.
Dani
Posts: 493
Joined: Mon Mar 10, 2003 3:17 pm
Contact:

Post by Dani »

Have you tried posting on a jewelry/metalsmithing board? Artists who work in Japanese metal blends like mokume gane could probably advise you ... also about milling the sheets to desired thickness.
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Post by Brad Walker »

Dani wrote:Have you tried posting on a jewelry/metalsmithing board? Artists who work in Japanese metal blends like mokume gane could probably advise you ... also about milling the sheets to desired thickness.
Good idea about posting on a metalsmithing board, I'll try that.

This isn't an isue of milling, as far as I can tell the material's only available in leaf, not in sheets. If I could find sheets, I'd be home free.
Ron Coleman
Posts: 468
Joined: Sun Mar 09, 2003 3:20 pm
Location: Columbus, Ohio USA

Post by Ron Coleman »

Sounds like it's copper or a copper alloy, aka "brass"

http://www.goldreverre.com/technique/gildingleaf.html

Try a little torch work on thin copper and see what happens, greens, purples,reds blues. Too much heat and "poof" it's gone
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Post by Brad Walker »

You're right, it's definitely an alloy with copper, just trying to figure out how what I need to mix with the copper to make some sheets of it.
Ron Coleman
Posts: 468
Joined: Sun Mar 09, 2003 3:20 pm
Location: Columbus, Ohio USA

Post by Ron Coleman »