I looked through the archives and the old archives for an answer to this question and didn't find one.
Did anyone ever gget a definitive answer as to whether micas are food safe or not? I'm playing with PearlEx micas and want to know if they're food safe, so I can label them properly.
Thanks -
Geri
Are micas food safe?
Moderators: Brad Walker, Tony Smith
-
Geri Comstock
- Posts: 340
- Joined: Mon Mar 10, 2003 4:16 pm
- Location: Northern CA
- Contact:
-
Tony Serviente
- Posts: 328
- Joined: Thu May 29, 2003 11:48 am
- Location: Ithaca,NY
- Contact:
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Both Aluminum and potassium silicate (mica) and titanium dioxide (colorant) are listed on the FDA's GRAS (Generally Recognized As Safe) list, and
"...may be safely used as colorants in the manufacture of articles or components of articles intended for use in producing, manufacturing, packing,
processing, preparing, treating, packaging, transporting, or holding food,..."
See US Code of Federal Regulations 21CFR178.3297
http://www.accessdata.fda.gov/scripts/c ... R=178.3297
Tony
ps: the FDA doesn't approve every application of every material. They have their GRAS list and specifically list applications that they are requested to approve. In this case, it's mica in contact with food and being used in a polymer based material. If you dig into the CFR, you'll find other approved applications for mica such as a colorant for contact lenses (direct wet body contact).
"...may be safely used as colorants in the manufacture of articles or components of articles intended for use in producing, manufacturing, packing,
processing, preparing, treating, packaging, transporting, or holding food,..."
See US Code of Federal Regulations 21CFR178.3297
http://www.accessdata.fda.gov/scripts/c ... R=178.3297
Tony
ps: the FDA doesn't approve every application of every material. They have their GRAS list and specifically list applications that they are requested to approve. In this case, it's mica in contact with food and being used in a polymer based material. If you dig into the CFR, you'll find other approved applications for mica such as a colorant for contact lenses (direct wet body contact).
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
-
Geri Comstock
- Posts: 340
- Joined: Mon Mar 10, 2003 4:16 pm
- Location: Northern CA
- Contact: