I've got some low fire dry enamels (thompson) to silkscreen on decal paper. If i use the Bullseye Glastac it won't work because its water soluble, I need to find a medium that will remain in tact while i submerge the decal paper in water. Paradise Paints fire to high. I'm wondering if acrylic medium will fire out ok. Any suggestions? 
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Enamel medium for waterslide decals
Squeegee oil from Thompson or Reusche or any other of many suppliers is what to use. it is a pine oil based formula made for silk screening or hand painting glass or china enamels.tsilvabarbosa wrote:I've got some low fire dry enamels (thompson) to silkscreen on decal paper. If i use the Bullseye Glastac it won't work because its water soluble, I need to find a medium that will remain in tact while i submerge the decal paper in water. Paradise Paints fire to high. I'm wondering if acrylic medium will fire out ok. Any suggestions?
I am slightly skeptical that the Thompson enamels are too coarse to work as decals. I can not tell you this for sure. Fine powder enamels do work though.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Not only a coarse screen, a metal mesh that won't get cut by the grit of the Thompson enamel. I've got the Thompson stuff, have done lots of screen printing and wouldn't dream of using them , 80 mesh,with a regular silk screen. Thompson's will make a finer mesh if you special order it but I suspect you will have a long learning curve You need what is called cover coat. Some are not designed to be used by a hand silk screener and will dry/plug the cover coat screen in 30 seconds. Kevin
-
Nelson Tan
- Posts: 41
- Joined: Sun Mar 09, 2003 9:23 pm
- Location: Manila
- Contact:
Hi. I did some experiment with enamel decals.
The Medium has to be compatible with the covercoat.
For screening enamel I use the polyester mesh 220 - 270.
For screening covercoat I use the 55 to 80 mesh.
Applying covercoat is the hardest part. It dries very quick and forms into web. I have to clean the screen every so often.
Hope this helps
Nelson
The Medium has to be compatible with the covercoat.
For screening enamel I use the polyester mesh 220 - 270.
For screening covercoat I use the 55 to 80 mesh.
Applying covercoat is the hardest part. It dries very quick and forms into web. I have to clean the screen every so often.
Hope this helps
Nelson