I recently received my new Paragon Fusion 7 and have had a ton of fun with it (can't wait to see my electric bill). I've done a few pieces with 2 to 3 levels of stacking using the firing instructions I found on this site. I now want to try something using more mosaic-like using one level. I was wondering if there is a chart somewhere with different firing schedules depending on the size of the piece and how many pieces of glass are being stacked. Any info would be greatly appreciated.
Thanks,
Stella
Newbie with question
Moderators: Brad Walker, Tony Smith
-
Lisa Allen
- Posts: 212
- Joined: Sun Mar 09, 2003 3:23 pm
- Location: Memphis, TN
- Contact:
Stella-
Glass seeks a 1/4", so if you only use one layer of 1/8th" pieces, it will draw up. Try using a clear base under your mosaic bits if you want the shape to retain its form.
Lisa
Glass seeks a 1/4", so if you only use one layer of 1/8th" pieces, it will draw up. Try using a clear base under your mosaic bits if you want the shape to retain its form.
Lisa
Lisa Allen
http://www.lisa-allen.com
Today's mighty oak is just yesterday's nut that held its ground.
http://www.lisa-allen.com
Today's mighty oak is just yesterday's nut that held its ground.