I've got blisters on me fingers
Moderators: Brad Walker, Tony Smith
-
Rocky Gentry
- Posts: 14
- Joined: Sun Mar 09, 2003 3:40 pm
- Location: St. Petersburg, FL
I've got blisters on me fingers
I have worn the fingers out of my Zetex gloves through the outer weave but not all the way through the lining. Is there anything I can wrap
the fingers with to get a bit more use out of them? Fireproof tape or something race car drivers or stunt men use? Thank you Hari Georgeson
for the title of the subject of this post.
the fingers with to get a bit more use out of them? Fireproof tape or something race car drivers or stunt men use? Thank you Hari Georgeson
for the title of the subject of this post.
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: I've got blisters on me fingers
There is always potholder mode.Rocky Gentry wrote:I have worn the fingers out of my Zetex gloves through the outer weave but not all the way through the lining. Is there anything I can wrap
the fingers with to get a bit more use out of them? Fireproof tape or something race car drivers or stunt men use? Thank you Hari Georgeson
for the title of the subject of this post.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Re: I've got blisters on me fingers
But ya gotta be quick! BlurBert Weiss wrote:There is always potholder mode.Rocky Gentry wrote:I have worn the fingers out of my Zetex gloves through the outer weave but not all the way through the lining. Is there anything I can wrap
the fingers with to get a bit more use out of them? Fireproof tape or something race car drivers or stunt men use? Thank you Hari Georgeson
for the title of the subject of this post.
My memory is so good, I can't remember the last time I forgot something . . .
-
Rocky Gentry
- Posts: 14
- Joined: Sun Mar 09, 2003 3:40 pm
- Location: St. Petersburg, FL
Bob wrote:Hi Rocky,
Tape for repairing mufflers?
The sash from your bath robe?
Cheers,
Bob
I fear that the flash tan ( on me nether parts ) from the lack of the sash on me bathrobe out weighs the danger of the blisters on me fingers. I will wrap all me parts in muffler repair tape ( whatever that is ) and tell you what got burnt and what didn't. If anything singes, I hold you responsible.
-
Brian and Jenny Blanthorn
- Posts: 353
- Joined: Mon Mar 10, 2003 5:25 pm
- Location: UK
- Contact:
Re: I've got blisters on me fingers
In the developement of Cunning Cheetin TechnologyRocky Gentry wrote:I have worn the fingers out of my Zetex gloves through the outer weave but not all the way through the lining. Is there anything I can wrap
the fingers with to get a bit more use out of them? Fireproof tape or something race car drivers or stunt men use? Thank you Hari Georgeson
for the title of the subject of this post.
I always go back 2 begining or B4 if I can
What R U doing ??
Meanwhile
Try painting glove with copydex but its gotta dry
U may wanna strengthen it with grit dusted on
I have cut out a lot of held grinding in numerous sneaky ways