Creating Depth

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
All Fired Up

Creating Depth

Post by All Fired Up »

Does anyone know how to achieve depth from simple shapes when fusing? Here are some examples:

Image

Image

Thanks,
Bartman
Phil Hoppes
Posts: 298
Joined: Wed Mar 12, 2003 2:20 pm
Location: Overgaard, AZ

Post by Phil Hoppes »

In art, that is called change in value. I would recommend practicing in an art medium first such as pencil drawing, pastels (my favorite), oils or acrylics. When you feel you have a handle on how to achieve the effect you are looking for in drawing then you should try working with powders in glass. They do not work like your drawing counterparts but it is as close as you can get. Be warned to be sure and always use a respirators when working with frits, especially powders as they are very bad for your lungs.

Good luck, happy drawing.

Phil
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Post by Bert Weiss »

read "The Art of Painting on Glass" by Albinus Elskus. This book shows how traditional glass painters create the effects you desire.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Don Burt
Posts: 580
Joined: Sun Mar 09, 2003 8:45 pm
Location: Bloomington, Indiana
Contact:

Re: Creating Depth

Post by Don Burt »

All Fired Up wrote:Does anyone know how to achieve depth from simple shapes when fusing? Here are some examples:

Image

Image

Thanks,
Bartman
I'm probably stating the obvious but in addition to value gradation like Phil was describing, depth is also acheived with linear perspective, variation in size of 2D shapes and density of texture, the illusion of pieces overlaying one another (theres a better phrase/word for that....darn) particularly with transparent class, and by actual physical depth itself. Different colors recede or approach too. You could get Rudolph Arnheim's big book from the library while you're waiting on Elskus's.
All Fired Up

Post by All Fired Up »

Don,

Which one of Rudolph's books are you talking about?
Don Burt
Posts: 580
Joined: Sun Mar 09, 2003 8:45 pm
Location: Bloomington, Indiana
Contact:

Post by Don Burt »

All Fired Up wrote:Don,

Which one of Rudolph's books are you talking about?
Sorry. He wrote a famous textbook in the '60s: Art and Visual Perception, A Psychology of the Creative Eye'.
Post Reply