Kiln atmosphere and devitrification
Hi, my name is Sean, I have question regarding the contamination of the atmosphere in an older kiln I’m using. I’m fusing Bullseye glass and have had devitrification problems. I put all new elements in the kiln, and am positive the kiln is powerful enough to reach desired temperatures at speeds that don’t cause devitrification. I'm also using alcohole to clean the glass. The kiln has been used for lots of different things, including kiln casting in plaster molds. Is there any way to clean the atmosphere, maybe by holding the kiln (empty) at a high temperature? Or is it a lost cause. Just a shot in the dark. Thanks Sean.
			
			
									
						
										
						- 
				The Hobbyist
- Posts: 311
- Joined: Sun Mar 09, 2003 7:09 pm
- Location: Sun City West (NW Phoenix), AZ
- Contact:
If you are using denatured alcohol it could be the additives they put in it. I have had devit-like streaks and I believe it is from the alcohol. I usually do a final cleaning wipe with it and I think that's where I'm getting the streaks.
I'm switching to rubbing alcohol or maybe even Everclear if it isn't too expensive.
The Hibbyist.........................................Jim
			
			
									
						
										
						I'm switching to rubbing alcohol or maybe even Everclear if it isn't too expensive.
The Hibbyist.........................................Jim
What kind of bullseye
Is it Bullseye fusible?  Are you mixing fusible and non-fusible Bullseye.  I have some green cathedral non-fusible bullseye that devits.  Charlie's right though.  Glass devits sometimes even when you regularly pay homage to the kiln gods . . .
AW
			
			
									
						
										
						AW
What kind of bullseye
Is it Bullseye fusible?  Are you mixing fusible and non-fusible Bullseye.  I have some green cathedral non-fusible bullseye that devits.  Charlie's right though.  Glass devits sometimes even when you regularly pay homage to the kiln gods . . .
AW
			
			
									
						
										
						AW
- 
				Sean Albert
- Posts: 8
- Joined: Wed Dec 10, 2003 7:04 pm
- Location: Alfred, NY
Yes it's Bulleye fusible and compatible, I called BE and they said once a kiln has been "contaminated" there is nothing you can do to fix, well they didn't know of any way to fix it, and suggested this website. I haven't had much luck with oversprays, is there one which is more highly recomended. Oh and I've been using isopropyle alcohol as recomended by lot's of people including BE to clean my glass before fusing. Thanks so much for the help so far, you guys are so fast!
Sean.
			
			
									
						
										
						Sean.
- 
				Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Seansean wrote:Yes it's Bulleye fusible and compatible, I called BE and they said once a kiln has been "contaminated" there is nothing you can do to fix, well they didn't know of any way to fix it, and suggested this website. I haven't had much luck with oversprays, is there one which is more highly recomended. Oh and I've been using isopropyle alcohol as recomended by lot's of people including BE to clean my glass before fusing. Thanks so much for the help so far, you guys are so fast!
Sean.
I'd try and clean your glass with a final cleaning using water and a good rub with a paper towel. The ideal paper towel is Bounty Microwave. It is supposedly guaranteed to not contain metal particles which can scratch.
I don't much about kiln contamination.
I recently did some testing of different glass cleaners. Sprayway foaming cleaner is a good one. You can get it from your local window glass shop or CR Laurence. I used a clear glass cleaner from the grocery store that worked well. I ran out and don't have the name in my head. The trick is to get a no ammonia formula.
Everclear works but at $19 a liter it is not a great economy. Especially as bottles have a way of getting smaller and smaller. It think it easily evaporates. Or something.
Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
I purchased a used ceramics kiln for fusing and everything I put in it had devit, plus it smelled terrible when fired.  Tried firing it empty really hot a couple of times to get rid of contamination without success.  Sold it to a potter for $100 more than I paid as it was no good for glass.  You might just need to find another kiln.
Carol
			
			
									
						
										
						Carol
- 
				Patty Gray
- Posts: 70
- Joined: Mon Mar 10, 2003 9:47 pm
- Location: Washington
- Contact:
Hi Sean,
Is it only certain colors or maybe only opals that show devit? If you are fusing with a glass that is prone to devit, either airbrushing or painting Super Spray onto the glass (let it dry before you fire) and you should be able to solve your devit problems. I find for cleaning glass I use just regular glass cleaner (no ammonia) and even on BE no problems. Some of the glass can be more prone to devit so if you make it a habit to clear cap or even use clear frit on top you can prevent the devit. Some only use Safeway glass cleaner. Different things work for different people.
I think what was causing Carol's problem in the old ceramic kiln was the use of some paints, lusters and such that will leave deposits on the elements. But you put new elements in so that shouldn't be the problem.
You might want to contact Rich at Kiln-tech @www.geocities.com/kilntec for some suggestions.
Good luck.
Patty
http://www.pattygray.com
			
			
									
						
										
						Is it only certain colors or maybe only opals that show devit? If you are fusing with a glass that is prone to devit, either airbrushing or painting Super Spray onto the glass (let it dry before you fire) and you should be able to solve your devit problems. I find for cleaning glass I use just regular glass cleaner (no ammonia) and even on BE no problems. Some of the glass can be more prone to devit so if you make it a habit to clear cap or even use clear frit on top you can prevent the devit. Some only use Safeway glass cleaner. Different things work for different people.
I think what was causing Carol's problem in the old ceramic kiln was the use of some paints, lusters and such that will leave deposits on the elements. But you put new elements in so that shouldn't be the problem.
You might want to contact Rich at Kiln-tech @www.geocities.com/kilntec for some suggestions.
Good luck.
Patty
http://www.pattygray.com
- 
				Brian and Jenny Blanthorn
- Posts: 353
- Joined: Mon Mar 10, 2003 5:25 pm
- Location: UK
- Contact:
In adittioncharlie wrote:glass devits. it's not the atmosphere (which gets replaced every time you open the lid) or anything to do with the kiln.
use an anti-devit spray and it should go away. search the archives for any number of solutions that can be used.
I vent the kiln till about 700 C
This gets rid of any smoky stuff which getrs on the glass n causes devit
If u got a few lifetimes spare there is a lot of devit stuff in the archives
An understanding of it will assist U in ur quest
Although there R those who actually like it
Brian

- 
				Amy Schleif-Mohr
- Posts: 280
- Joined: Sun Mar 09, 2003 5:18 pm
- Location: Milwaukee
Exactly what I figured...was figuring some of those impurities also be in/on the bricks as well as the elements.Patty Gray wrote:
I think what was causing Carol's problem in the old ceramic kiln was the use of some paints, lusters and such that will leave deposits on the elements. But you put new elements in so that shouldn't be the problem.
C.
- 
				Patty Gray
- Posts: 70
- Joined: Mon Mar 10, 2003 9:47 pm
- Location: Washington
- Contact:
Hi Brock, 
Yes when I fuse with BE or when my students fuse with BE they use regular glass cleaner. I use to use Sprayway but pretty much stopped after Avery said it caused devit on BE. I never experienced the devit from Sprayway but thought it would be a good change. Really the only time I experience true devit is with float glass and I always use Superspray with that (airbrush it on, let it dry).
Have fun with your Hawaiian classes, sounds great.
Patty
http://www.pattygray.com
			
			
									
						
										
						Yes when I fuse with BE or when my students fuse with BE they use regular glass cleaner. I use to use Sprayway but pretty much stopped after Avery said it caused devit on BE. I never experienced the devit from Sprayway but thought it would be a good change. Really the only time I experience true devit is with float glass and I always use Superspray with that (airbrush it on, let it dry).
Have fun with your Hawaiian classes, sounds great.
Patty
http://www.pattygray.com
- 
				Bob
- Posts: 215
- Joined: Mon Mar 10, 2003 1:01 pm
- Location: Salt Spring Island, British Columbia
- Contact:
Sean,
I think taking the kiln to a high temperature and trying to burn off any contaminants is a good idea. If it is a ceramic kiln it will probably go to well above 2000F which is well above the working temperature for glass. Vent the kiln so the contaminants have a chance to escape.
I am surprised that the overglaze doesn't help... it should provide a protective coating. Also try firing quickly through the temp range that promotes devitrification... starting at 1375F.
Replace your kiln goddess... she ain't pulling her weight.
Cheers,
Bob
			
			
									
						
										
						I think taking the kiln to a high temperature and trying to burn off any contaminants is a good idea. If it is a ceramic kiln it will probably go to well above 2000F which is well above the working temperature for glass. Vent the kiln so the contaminants have a chance to escape.
I am surprised that the overglaze doesn't help... it should provide a protective coating. Also try firing quickly through the temp range that promotes devitrification... starting at 1375F.
Replace your kiln goddess... she ain't pulling her weight.
Cheers,
Bob
I agree that before giving up on the kiln to fire it as hot as you can and vent the fumes.  I would be surprised if you still have a problem afterwards. Lots of things can contaminate a kiln including wax from casting molds if it was used as a burn-out oven.... but, few things are so resistent that they won't burn off at a high enough temperature. Don't give up quite yet.  And just for the record, I wasted way too much glass a few years ago believing the "won't devit" advertising.  Do yourself a favor and just use an overspray on every glass.  You won't even have to vent the kiln tbrough the nasty temp range.  I use superspray or borax solution and just make sure you fuse at a high enough temp to avoid blotches.  There's not a need to spray a second time and don't make the mistake of applying during a slump.  Good luck!
			
			
									
						
										
						- 
				daffodildeb
- Posts: 125
- Joined: Mon Jul 28, 2003 3:48 am
- Location: Hot Springs Village, AR
- 
				Amy Schleif-Mohr
- Posts: 280
- Joined: Sun Mar 09, 2003 5:18 pm
- Location: Milwaukee
- 
				Bev Brandt
- Posts: 50
- Joined: Mon Mar 10, 2003 11:35 am
- Location: St. Louis, MO
- Contact:
You know...my *neighbor* asked me about my kiln goddess. Which is odd considering my neighbor is a public health policy professor. Perhaps his wife - an ex-fiber artist - had a Loom Goddess.Bob wrote:Replace your kiln goddess... she ain't pulling her weight.
Do these god and goddesses come to you or do you have to create them? I have some old Barbies around, perhaps one would like a promotion.
- Bev
Bev Brandt
			
						- 
				Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Old Barbies are excellent. Recycling is very much encouraged this millennium. Smudge her with sage and she's in.Bev Brandt wrote:You know...my *neighbor* asked me about my kiln goddess. Which is odd considering my neighbor is a public health policy professor. Perhaps his wife - an ex-fiber artist - had a Loom Goddess.Bob wrote:Replace your kiln goddess... she ain't pulling her weight.
Do these god and goddesses come to you or do you have to create them? I have some old Barbies around, perhaps one would like a promotion.
- Bev
Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions