Does anyone have positive or negative experiences using this glue to glue on findings? Where do you find this glue?
			
			
									
						
										
						- 
				Tony Serviente
 - Posts: 328
 - Joined: Thu May 29, 2003 11:48 am
 - Location: Ithaca,NY
 - Contact:
 
Home Depot type store, or preferably a good local hardware store will have it, or some type of polyurethane glue. Any brand will work. Pro is the bonding strength and the variety of materials it will work with. Con is that it does not cure clear, but brown, and the cure time is hours long. It also expands when curing which can cause problems if you don't account for it. Also is a mess to clean up if it gets on anything you don't want to be on, like skin.