kiln element proximity to insulation
Moderators: Brad Walker, Tony Smith
- 
				Phil Hoppes
 - Posts: 298
 - Joined: Wed Mar 12, 2003 2:20 pm
 - Location: Overgaard, AZ
 
Tony,
I think we are saying the same thing. The Paragon elements are in a fiber not a cement btw. Not sure how they do that, I'm guessing it is a slurry of some type with fiber and when it dries the elements are then embedded inside of the material. Anyway, it make a much nicer ceilling than brick as it does not rain on my glass.
Phil
			
			
									
						
										
						I think we are saying the same thing. The Paragon elements are in a fiber not a cement btw. Not sure how they do that, I'm guessing it is a slurry of some type with fiber and when it dries the elements are then embedded inside of the material. Anyway, it make a much nicer ceilling than brick as it does not rain on my glass.
Phil
- 
				Tony Serviente
 - Posts: 328
 - Joined: Thu May 29, 2003 11:48 am
 - Location: Ithaca,NY
 - Contact:
 
I have Kanthal elements on mullite cores. Some are up tight against fiber board, others have an inch or more air clearance, and there is no difference in failure rate over a period of years and thousands of firings. In fact, the failures of the elements always come down to either the connections, or corrosion from glass. Have never had one "burn out".
			
			
									
						
										
						heat buildup because of lack of heat conduction away from the element? or relection of heat back onto the element? it will be hotter than the rest of the kiln space, but perhaps not hotter than the element itself.Brock wrote:Not in my experience. I had to add some insulation to the roof of one of my kilns, and the element has been in contact with the ceri-wool for years. Now, two of them are like that. No problem. Anyway, I've never understood what you just proposed. The element is the hottest thing in the kiln, how can it get hotter by touching insulation? Mr. Science
- 
				Bert Weiss
 - Posts: 2339
 - Joined: Tue Mar 11, 2003 12:06 am
 - Location: Chatham NH
 - Contact:
 
PhilPhil Hoppes wrote:Bert,
I'm using nichrome elements both in quartz tubes for the top and mullite rods with doughnut supports for the sides. Joppa's been selling these elements longer than I think I've been alive without people having problems so I don't think, for nichrome and fiber insulation, touching at least on one side is a problem.
Phil
Your design has a BIG PROBLEM. I looked in to using quartz tubes and nichrome elements and was told by Duralite that they are not compatible. The nichrome gives off an oxide that will coat the inside of the quartz and significantly lower it's efficiency. Kanthal doe not have this problem.
You could wind the coils around the quartz.
Most pottery kilns use kanthal because it can take higher temps. A Kanthal element can drive a kiln up to 2300º. Nichrome is only good to somewhere around 1900 or so.
Bert
Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
- 
				Phil Hoppes
 - Posts: 298
 - Joined: Wed Mar 12, 2003 2:20 pm
 - Location: Overgaard, AZ
 
Bert,
The elements in the quartz tubes are the elements sold to me by Duralite. I do not know the exact material, I was just assuming that they are nichrome, but I have to believe that they are compatiable with the quartz as this is what Duralite sells as a set. If nichrome and quartz don't work, then I'm guessing that the top elements are probably kanthal. I'll look into it since you mention it. The side elements I know are nichrome. [update. They are kanthal inside the quartz tubes. The side elements are nichrome but I don't think they should pose an issue with the quartz tubing.]
Phil
			
			
									
						
										
						The elements in the quartz tubes are the elements sold to me by Duralite. I do not know the exact material, I was just assuming that they are nichrome, but I have to believe that they are compatiable with the quartz as this is what Duralite sells as a set. If nichrome and quartz don't work, then I'm guessing that the top elements are probably kanthal. I'll look into it since you mention it. The side elements I know are nichrome. [update. They are kanthal inside the quartz tubes. The side elements are nichrome but I don't think they should pose an issue with the quartz tubing.]
Phil
- 
				Bert Weiss
 - Posts: 2339
 - Joined: Tue Mar 11, 2003 12:06 am
 - Location: Chatham NH
 - Contact:
 
PhilPhil Hoppes wrote:Bert,
The elements in the quartz tubes are the elements sold to me by Duralite. I do not know the exact material, I was just assuming that they are nichrome, but I have to believe that they are compatiable with the quartz as this is what Duralite sells as a set. If nichrome and quartz don't work, then I'm guessing that the top elements are probably kanthal. I'll look into it since you mention it. The side elements I know are nichrome. [update. They are kanthal inside the quartz tubes. The side elements are nichrome but I don't think they should pose an issue with the quartz tubing.]
Phil
You are probably fine. They most likely sold you Kanthal for the quartz. I see no reason why you can't run differrent elements at once. I'm glad to hear that you don't have the wrong stuff.
Whatever Paragon used to enclose the elements is special stuff that obviously works. Just because it is soft doesn't insure that it is not an insulator. It would have to be a radiator in order to make sense as a system. (Does that mean that you need antifreeze in it?)
I tried to get set up with nichrome and quartz or straight wire elements, quartz and Kanthal, but neither system met proper standards.
Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
- 
				Phil Hoppes
 - Posts: 298
 - Joined: Wed Mar 12, 2003 2:20 pm
 - Location: Overgaard, AZ
 
- 
				Tony Smith
 - Posts: 1037
 - Joined: Sun Mar 09, 2003 5:59 pm
 - Location: Massachusetts, USA
 - Contact:
 
- 
				Keith Barnett
 - Posts: 3
 - Joined: Wed Dec 10, 2003 6:04 am
 - Location: The Summit, Queensland, Australia.
 
Top hat kilns
Greg,
There's a guy who lives at Crib Point on the Mornington Peninsula called Peter Riley who makes top hat kilns. He may be able to give you some advice. If you can't find his number let me know.
			
			
									
						
							There's a guy who lives at Crib Point on the Mornington Peninsula called Peter Riley who makes top hat kilns. He may be able to give you some advice. If you can't find his number let me know.
Cheers,
           
Keith.
Firetail Glass,
Qld, Australia.
			
						Keith.
Firetail Glass,
Qld, Australia.
- 
				Hugo Gavarini
 - Posts: 49
 - Joined: Mon Mar 10, 2003 12:03 pm
 - Location: Patagonia Argentina
 
My two cents,
Kanthal A1 is magnetic while Nichrome is not.
The rate of power delivery from the element at high temperatures will be proportional to the differences between element temperature and medium temperature both to the fourth power:
Energy Delivered ~ (Telement)exp 4 - (Tmedium)exp 4
So, if you consider the insulation as the targeted medium and it is close to the element, that difference will be almost inexistent. So, your element will release far more energy from the "free" sector of the coil (to the kiln interior and to the glass). The only drawback would be the ceramic fiber crystallization (changing from amorphous to crystobalite crystals) at such high temperature becoming locally brittle and a health hazard. I believe it's not alternative to this lay-out for the elements. Perhaps we shall learn to live together with these issues.
			
			
									
						
							Kanthal A1 is magnetic while Nichrome is not.
The rate of power delivery from the element at high temperatures will be proportional to the differences between element temperature and medium temperature both to the fourth power:
Energy Delivered ~ (Telement)exp 4 - (Tmedium)exp 4
So, if you consider the insulation as the targeted medium and it is close to the element, that difference will be almost inexistent. So, your element will release far more energy from the "free" sector of the coil (to the kiln interior and to the glass). The only drawback would be the ceramic fiber crystallization (changing from amorphous to crystobalite crystals) at such high temperature becoming locally brittle and a health hazard. I believe it's not alternative to this lay-out for the elements. Perhaps we shall learn to live together with these issues.
Hugo
			
						- 
				Tony Serviente
 - Posts: 328
 - Joined: Thu May 29, 2003 11:48 am
 - Location: Ithaca,NY
 - Contact:
 
- 
				Hugo Gavarini
 - Posts: 49
 - Joined: Mon Mar 10, 2003 12:03 pm
 - Location: Patagonia Argentina
 
Tony,
According to my notes, the temperature in which ceramic refractories bearing amorphous silica start the transformation to crystalline silica is 1000°C or 1832°F. That is below 1260°C or 2300°F, the maximum working temperature for IFB.
That's why I have chosen 980°C or 1796°F as my normal operation maximum temperature.
BTW, the maximum operative temperature for Kanthal A1 diameter 1.3mm. is 1186°C or 2167°F. According to my calculations, the element temperature for 980°C (1796°F) is 1088°C or 1990°F, so I think my elements will last a lot of firings. It would be interesting to notice that the maximum temperature for a kiln is not only established by the refractory material but for the heating element properties and lay-out too.
			
			
									
						
							According to my notes, the temperature in which ceramic refractories bearing amorphous silica start the transformation to crystalline silica is 1000°C or 1832°F. That is below 1260°C or 2300°F, the maximum working temperature for IFB.
That's why I have chosen 980°C or 1796°F as my normal operation maximum temperature.
BTW, the maximum operative temperature for Kanthal A1 diameter 1.3mm. is 1186°C or 2167°F. According to my calculations, the element temperature for 980°C (1796°F) is 1088°C or 1990°F, so I think my elements will last a lot of firings. It would be interesting to notice that the maximum temperature for a kiln is not only established by the refractory material but for the heating element properties and lay-out too.
Hugo
			
						:?:Tony Smith wrote:Bert Weiss wrote: you end up with a mini China Syndrome and the element melts down.
Tony
I wonder if that phrase's meaning will ever become a trivia question, like "lock stock and barrel" the 3 parts needed to complete a flint lock firearm, who's components could be bought separatley, or all at once, Lock stock and barrel.
Cliff Claven
I didn't consider it that way before, Cliff -it's always interesting to hear someone else's interpretation.Liam wrote:Tony Smith wrote:Bert Weiss wrote: you end up with a mini China Syndrome and the element melts down.
Tony![]()
I wonder if that phrase's meaning will ever become a trivia question, like "lock stock and barrel" the 3 parts needed to complete a flint lock firearm, who's components could be bought separatley, or all at once, Lock stock and barrel.
Cliff Claven
Mine is; if you get something lock, stock and barrel, it means you get the key to the door (the lock), the stock (everything in the shop) and the barrel (you need a license to sell licquor, so it includes anything alcoholic in the place)!
and if somebody gets it lock, stock and two smoking barrels, it means they blasted their way in to take everything!
It ain't where you're from, it's where you're at!