bowls are not shiny on their rims after I slump them..Help

Post by deborahbur »

I have tried most everything. My round rice style bowls are fine on their edges when I fuse them but get cloudy when I slump them? Any ideas?\

Thanks
Deborah
Bowls are 7" across flat
jerry flanary
Posts: 158
Joined: Tue Sep 09, 2003 11:11 pm
Location: norfolk, va

Post by jerry flanary »

Do you have this trouble w/ all color combos? Is it devit? Have you invested in a cold shop?
j.

A lack of doubt doesn't lend certainty.
Barbara Muth
Posts: 382
Joined: Sun Mar 09, 2003 8:10 pm
Location: Washington DC Metropolitan Area
Contact:

Post by Barbara Muth »

is the first firing on thinfire?
Barbara
Check out the glass manufacturer's recommended firing schedules...
LATEST GLASS
deborahbur
Posts: 51
Joined: Thu Apr 10, 2003 2:09 pm
Location: Tiverton, Rhode Island
Contact:

Post by deborahbur »

All colors are cloudy around the top.......yes the first firing was on thin fire.

What kind of cold work?

Thanks
Deborah