No, this one is hot cast; if you see clear glass of good transparency in my work then it is hot cast. Kiln sand cast are "Castle made of sand 1&2", "The Hut of Baba Yaga", the 2 center objects of "Reflections of the past:Remains of human history" and "Space Architecture"glassburl wrote:
Lucho,
I went to your website and looked around. This method of kiln sand casting you use, did you use it to cast "17 Houses of the Holy 5" for instance?
Hugh
annealing schedules for large kiln cast sculptures
Moderator: Brad Walker
-
lucho/lachezar/
- Posts: 15
- Joined: Tue Aug 03, 2004 12:46 pm
- Location: bulgaria
- Contact: