This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.
Moderators: Brad Walker , Tony Smith
fun5oh
Posts: 32 Joined: Mon Dec 15, 2003 11:30 pm
Location: wisconsin
Post
by fun5oh » Sat Dec 20, 2003 10:56 pm
Probably a dumb question, but I am going to ask anyways. Can I put a freshly kiln washed mold on the kiln floor to dry, while I am fusing pieces on a shelf above it?
Thanks,
Robin
Brock
Posts: 1519 Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.
Post
by Brock » Sat Dec 20, 2003 10:58 pm
Yup. Brock
fun5oh
Posts: 32 Joined: Mon Dec 15, 2003 11:30 pm
Location: wisconsin
Post
by fun5oh » Sun Dec 21, 2003 12:21 am
Is that "Yup" I can dry it or "Yup" it's a dumb question?
Robin
Brock
Posts: 1519 Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.
Post
by Brock » Sun Dec 21, 2003 12:32 am
Yup, you can dry it. Brock