kiln wash

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
fun5oh
Posts: 32
Joined: Mon Dec 15, 2003 11:30 pm
Location: wisconsin

kiln wash

Post by fun5oh »

Probably a dumb question, but I am going to ask anyways. Can I put a freshly kiln washed mold on the kiln floor to dry, while I am fusing pieces on a shelf above it?

Thanks,
Robin :)
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Post by Brock »

Yup. Brock
fun5oh
Posts: 32
Joined: Mon Dec 15, 2003 11:30 pm
Location: wisconsin

Post by fun5oh »

Is that "Yup" I can dry it or "Yup" it's a dumb question?

Robin :)
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Post by Brock »

Yup, you can dry it. Brock
Post Reply