			WildHeart999 wrote:Thanks for all the suggestions.  What is pink striker?
Connie
Jerry Cave wrote:dvallere wrote:Anybody tried CBS's "Candy Apple Red"?  That SOUNDS like it ought to really be the stuff, but...I haven't tried it yet. 
D.
Yep.  Cap it with pink striker...
 
 
pink striker is a color from bullseye, it "strikes" to a nice pink color during firing, before firing looks very pale blue.  color #1215
D
 
		 
				
		
		 
	 
				
		
		
			- 
				
																			 Jerry Cave
- Posts: 78
- Joined: Tue Mar 11, 2003 2:59 pm
- Location: Zig Zag Oregon
						
					
													
							
						
									
						Post
					
								by Jerry Cave » 
			
			
			
			
			
pink striker is a color from bullseye, it "strikes" to a nice pink color during firing, before firing looks very pale blue.  color #1215
D
Yes indeed.  And it certainly influences that candy apple into a very nice red. 
jerry
 
		 
				
		
		 
	 
				
		
		
			- 
				
																			 Dolores
- Posts: 106
- Joined: Mon Jul 14, 2003 9:21 pm
- Location: Sunny Southern California
- 
				Contact:
				
			
						
					
													
							
						
									
						Post
					
								by Dolores » 
			
			
			
			
			You can also get a nice red by fusing clear candy apple red coating side down over black glass.
DOLORES