WildHeart999 wrote:Thanks for all the suggestions. What is pink striker?

Connie
Jerry Cave wrote:
dvallere wrote:Anybody tried CBS's "Candy Apple Red"? That SOUNDS like it ought to really be the stuff, but...I haven't tried it yet.

D.

Yep. Cap it with pink striker...
pink striker is a color from bullseye, it "strikes" to a nice pink color during firing, before firing looks very pale blue. color #1215
D
Dee Janssen
Unicorn's Creations Studio
http://ucjewelry.com
dee@ucjewelry.com
Jerry Cave
Posts: 78
Joined: Tue Mar 11, 2003 2:59 pm
Location: Zig Zag Oregon

Re: True Red Dichroic

Post by Jerry Cave »


pink striker is a color from bullseye, it "strikes" to a nice pink color during firing, before firing looks very pale blue. color #1215
D

Yes indeed. And it certainly influences that candy apple into a very nice red.



jerry
Dolores
Posts: 106
Joined: Mon Jul 14, 2003 9:21 pm
Location: Sunny Southern California
Contact:

Re: True Red Dichroic

Post by Dolores »

You can also get a nice red by fusing clear candy apple red coating side down over black glass.