You are so still needed
What would you charge a contractor to blast, for his customer, one surface of 6, 46" x 8-1/2" pieces of 3/8" float (for shelving).
I blasted a scrap piece that size last night to make sure I could get an even finish (in a 48" dia cabinet) and it came out nice and even. I told him this morning it would be $150 for the job, and he was happy.
I didn't know whether to charge by the job or by the hour for this kind of thing.
Nikki