I'm asking this for my Girl.
Should she slump a piece first and then on the next firing do the tacking? Or can both be done at the same time?
The husband.
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Post by Brock »

Neither. Tack, then slump. Brock