This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.
Moderators: Brad Walker, Tony Smith
-
Compton
- Posts: 2
- Joined: Mon Dec 22, 2003 12:25 pm
Post
by Compton »
I'm asking this for my Girl.
Should she slump a piece first and then on the next firing do the tacking? Or can both be done at the same time?
The husband.
-
Brock
- Posts: 1519
- Joined: Mon Mar 10, 2003 1:32 pm
- Location: Vancouver, B.C.
Post
by Brock »
Neither. Tack, then slump. Brock